Super Duplex S32760 / F55 yeeb nkab
JN Alloy yog tus xa khoom thiab chaw tsim khoom uas muab S32760 duplex steel khoom, S32760 duplex steel yeeb nkab thiab Tubes, ASTM A790 UNS S32760 Tube, 1.4501 Tube, S32760 Yeeb Nkab, S32760 Khoom, S32760 Nqe, S32.
UNS S32760 Pipes yog super duplex kav ua los ntawm 50:50 piv ntawm austenitic thiab ferritic microstructure. Cov hlau no sib xyaw ua ke siab txhua yam muaj zog thiab zoo ductility nrog zoo corrosion kuj. Cov kav dej no feem ntau muab nkag rau hauv cov txheej txheem annealed nrog lub zog tawm ntawm 550 MPA. Cov kav dej no tsis tuaj yeem hardened los ntawm cov txheej txheem kev kho cua sov tab sis lub zog siab yog ua tiav los ntawm cov txheej txheem ua haujlwm txias. Cov kav dej no tau muab nrog pitting tsis kam sib npaug uas ua kom muaj siab pitting corrosion kuj. Tsis tas li ntawd, nws yog ua ke nrog crevice thiab kev nyuaj siab corrosion cracking nrog ntxiv zog. Thaum UNS S32760 cov kav dej txias tau kos nws pom qhov xwm txheej sib nqus. Tsis tas li ntawd, cov kav dej no muaj qhov zoo thermal stability thiab conductivity. Qhov no alloy yog paub rau nws formability, ntaub muaj peev xwm, thiab machinability. Txhua yam txheej txheem vuam siv tau rau vuam cov kav dej no. Qhov no feem ntau yog vim qhov siab molybdenum, chromium, thiab nitrogen cov ntsiab lus hauv Sa 790 Uns S32760 Tube. Qhov kub ntawm qhov sib cuam tshuam yuav tsum tsis txhob ntau tshaj 100 ° C hauv qhov vuam kom tiv thaiv cov khoom sib txuas.
Jinie Technology (Jiangsu) Co., LTD yog lub chaw tsim khoom tshwj xeeb los muab nws cov neeg siv khoom zoo tshaj plaws ntawm cov nqi sib tw thiab tseem muaj cov kev pabcuam xa khoom sai tshaj plaws. Peb tau cuv npe nrog cov qauv hauv tebchaws thiab thoob ntiaj teb txhawm rau ua kom tiav daim ntawv thov kev xav tau ntawm cov neeg siv khoom.
Peb khaws cov kav dej no nyob rau hauv ntau yam qauv, specifications, qhov ntev thiab txiav lengths. Cov neeg siv khoom kuj tuaj yeem thov lwm yam kev xav tau tshwj xeeb raws li lawv daim ntawv thov xav tau. Tsis tas li ntawd, cov kav dej no tau muab los ntawm cov txheej txheem sib tsoo rau qhov tseeb qhov tseeb thiab qhov chaw tiav. Ntawm qhov tshwj xeeb xav tau ntawm cov neeg siv khoom, peb polish UNS S32760 Pipes nrog cov tsho loj los ntxiv kev tiv thaiv los ntawm xeb hauv qhov chaw tsis zoo. Hauv peb cov khoom, txhua Super Duplex S32760 Tubes yog tsim los ntawm cov khoom siv raw khoom zoo. Tsis tas li ntawd, lawv ua qee qhov kev ntsuam xyuas zoo los xyuas kom meej qhov zoo ntawm Tubes. Peb ntim peb Cov Tubes hauv cov khoom zoo kom paub tseeb tias kev tiv thaiv kev puas tsuaj. Nrog rau peb lub network faib dav thiab kev thauj mus los zoo, peb muaj peev xwm muab peb Cov Tubes ntawm txhua lub ces kaum ntawm lub tebchaws. Peb xa peb cov Orders raws sijhawm yam tsis muaj kev ncua.
Standard Specification rau Super Duplex Steel S32760 Pipes & Tubes
|
Cov qauv |
ASTM / ASME A790, A928, A789 / SA790, SA928, SA789 |
|
Sab nraud |
6.00 hli OD txog 914.4 hli OD, Qhov ntau thiab tsawg mus txog 24 "NB |
|
Thickness |
0.3mm-50mm |
|
Hom |
Seamless / ERW / EFW / Welded / Fabricated / LSAW Pipes |
|
Teem caij |
TXC 20 SCH 30 SCH 40 STD SCH 80 SCH 60 SCH 80 SCH 120 SCH 140 SCH 160 XXS |
|
Seamless Pipes & Tubes Loj |
1/8 "NB-24" NB |
|
ERW Pipes & Tubes Loj |
1/8 "NB-36" NB |
|
EFW Pipes & Tubes Loj |
6" NB - 100" NB |
|
Ntev |
Ib qho Random, Ob Chav Random & Ntev Ntev |
|
Daim ntawv |
Round Pipes/Tubes, Square Pipes/Tubes, Rectangular Pipes/Tubes, Coiled Tubes, "U" Shape, Pan Cake Coils, Hydraulic Tubes |
|
Xaus |
Plain End, Beveled End, Threaded |
Super Duplex Steel S32760 Pipes & Tubes Tshuaj Chemical Composition
|
Qib |
C |
Mn |
Si |
P |
S |
Cr |
Mo |
Ni |
N |
Fe |
|
S32760 |
0.05 max |
max 1.00 Nws |
max 1.00 Nws |
0.030 max |
0.010 max |
24.00 – 26.00 |
3.00 – 4.00 |
6.00 – 8.00 |
0.20 – 0.30 |
5 7,61m |
Mechanical Properties ntawm Super Duplex Steel S32760 Yeeb thiab Tubes
|
Qib |
Qhov ceev (g / cm3) |
Qhov ceev (lb / hauv 3) |
Melting Point (zeeg) |
Melting Point (° F) |
|
S32760 |
7.8 |
0.281 |
1350 |
2460 |
Super Duplex stainless hlau S32760 Qib sib npaug
|
STANDARD |
WERKSTOFF NR. |
UNS |
EN |
|
Super Duplex S32760 |
1.4501 |
S32760 |
X2CrNiMoCuWN25-7-4 |
Daim ntawv thov Super Duplex F55 yeeb nkab
Super Duplex Steel UNS S32760 cov kav dej, feem ntau hu ua duplex stainless hlau hlab, nrhiav kev siv dav. Lawv cov khoom zoo heev thiab kev tiv thaiv corrosion ua rau cov kav dej duplex stainless hlau tsim rau ntau yam kev siv; Nov yog qee qhov kev siv ntau yam:
1. Kev lag luam roj thiab roj:Super Duplex Steel S32760 cov kav dej tau dhau los siv thoob plaws hauv cov roj thiab cov roj siv rau kev siv ntawm ntug dej hiav txwv, cov kav dej hauv qab thiab cov chaw ua haujlwm, vim lawv lub zog zoo heev - tus yam ntxwv corrosion - zoo tagnrho rau cov cheeb tsam hnyav nrog cov kua dej ntau heev uas xav tau kev tiv thaiv.
2. Kev ua tshuaj lom neeg:Cov kav dej S32760 no feem ntau pom muaj nyob rau hauv cov chaw ua tshuaj uas tiv thaiv corrosion los ntawm ntau yam tshuaj, acids, thiab cov kuab tshuaj yog qhov tseem ceeb. Lawv pom muaj nyob rau hauv reactors, heat exchangers, cia tank thiab piping systems raws li tus nqi - txiav kev ntsuas.
3. Kev siv Marine:Ua tsaug rau lawv cov kev tiv thaiv corrosion nyob rau hauv marine ib puag ncig, Super Duplex Steel S32760 kav dej pom siv nyob rau hauv shipbuilding, offshore structures thiab pipeline systems.
4. Kev tsim kho thiab Architecture:Super Duplex Steel S32760 cov kav dej tau dhau los ua cov khoom siv dav dav rau cov qauv vaj tsev zoo li txuas hniav thiab cov tsev uas muaj kev tiv thaiv corrosion thiab kev zoo nkauj yog qhov tseem ceeb heev.
5. Cov Chaw Kho Dej:Cov kav dej S32760 no feem ntau ua haujlwm ntawm cov chaw kho dej kom nyab xeeb thauj cov kua ntau yam xws li tshuaj thiab dej kho vim lawv muaj peev xwm tiv taus corrosion thiab yaig.
6. Automotive thiab Aerospace:Super Duplex Steel S32760 cov kav dej tuaj yeem pom cov ntawv thov hauv tsheb thiab aerospace daim ntawv thov uas muaj zog, corrosion kuj thiab lub teeb yuag tau nrhiav tawm - piv txwv li hauv cov ntawv thov uas muaj zog, tiv thaiv corrosion, lub teeb yuag yog qhov tseem ceeb - xws li cov tsheb sib kis kab.
Super Duplex Steel UNS S32760 cov kav dej tau dhau los siv dav hauv kev lag luam uas hais txog kev tiv thaiv corrosion, lub zog thiab kav ntev raws li cov kev cai tseem ceeb rau cov khoom lossis cov tshuab.