JN Alloy yog loj tshaj plaws ntawm cov hlau uas muaj hluav taws xob loj tshaj plaws ntawm cov khoom lag luam loj: ASTM AISI 321 kub lub phaj ntawm AISI31 kub UNNT Phaj thiab 321 Hlau Txias Cug Ntawv. Peb muab DIN 1.4541 coils hauv ntau qhov ntau thiab tsawg ntawm tus nqi zoo tshaj plaws. Peb yog cov qauv tsim khoom lag luam ntawm 321 steel sawb & SS 321 daim ntawv.
321 Daim Ntawv Hlau Stainless Hlau yog lub titanium stabilized austenitic chromium-npib tsib}}} Hom alloy nrog kev txhim kho intergrraneular-corrosion tsis kam. Cov khoom siv no yog stabilized tawm tsam chromium carbide tsim los ntawm kev ntxiv ntawm titanium. Txij li titanium muaj ib qho muaj zog rau cov pa roj carbon ntau dua li chromium, titanium carbide precipitates nyob rau hauv kev sib sau ua ib thaj chaw nplej. Lub 321 stainless hlau phaj yog ua los ntawm Austenitic Stainless hlau uas muaj Titanium ua lub stabilizer. Qhov no feem ntau siv rau cov ntawv thov uas kub yog ib qho ntawm cov teeb meem loj. Lawv tuaj yeem siv tau zoo nyob rau hauv cov kev pabcuam uas nws kub nce mus txog 900 degrees tsis muaj zog rau cov khoom siv hluav taws xob sib txawv, tshwj xeeb yog qhov xav tau cov khoom siv sib txawv ntawm 800ºF (427ºC) thiab 1650ºF (899C), lossis rau vuam raws cov xwm txheej uas tiv thaiv tus post-weld anneal.
A ISO 9001: 2008 Cov Tuam Txhab Pov Thawj, jn alloy yog ib qho khoom lag luam, tus xa khoom thiab cov xa khoom ntawm Astm ib {2}} stainless hlau daim hlau. ASTM 240 321} Cov paib hlau stainless yog txiav rau koj cov specifications kom zoo thiab muab tau tiav teeb tsa ntawm cov ntawv xeem zeb. Kev cai ntev thiab dav mus txog 2000 mm tuaj yeem ua tau. Kev xa tawm yog peb tshwj xeeb! Thiab peb tuaj yeem ntsib ntau yam nyuaj los nrhiav qib thiab lossis cov qauv tsis muaj ntau thiab tsawg kom tau raws li qhov tshwj xeeb ntawm peb cov neeg siv khoom. Txhua ASTM 240 321} Cov paib hlau stainless tuaj yeem txiav rau qhov loj nrog kev pab ntawm peb cov kev txawj ntse ntau hauv kev ua cov khoom lag luam steel. Peb muab 321 stainless hlau ntawv nyob rau ntau qhov ntev thiab dav thiab tuaj yeem tsim kev txiav rau koj cov lus qhia tseeb. Lub stainless hlau 321 lub phaj muaj nyob nrog customizable qhov ntev thiab ntau thiab tsawg. Lawv cov npoo av ua tau kuj tuaj yeem txhim kho cov tsos thiab corrosion resistance muaj ntawm cov khoom. Lawv yog qhov yooj yim ua ke raws li cov kev cai tshwj xeeb.
AISI 321 daim ntawv phaj tshwj xeeb
|
Cov lus qhia |
ASTM A240 / ASME SA240 |
|
Kev Pom Zoo Duaensional |
JIS, AISI, ASSM, GB, DIN, EN, ETC |
|
Qhov dav |
1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500 hli, 3000mm, 3500mm, thiab lwm yam |
|
Qhov tuab |
4 hli -100 hli |
|
Qho ntev |
2000mm, 2440mm, 3000mm, 5800mm, 6000mm, thiab lwm yam |
|
Nto tas |
2b, 2d, BA, No.1, No.4, 8K, Duab, etching, kub dov phaj (CR), satin (tau ntsib nrog yas coated) thiab lwm yam. |
|
Kev nyuaj |
Mos, nyuaj, ib nrab nyuaj, peb lub hlis twg nyuaj, lub caij nplooj ntoo hlav zog thiab lwm yam. |
|
Puab |
Coils, ntawv ci, yob cov ntawv dawb, shim ntawv, phaj perforated, sawb, dawb paug (flange) thiab lwm yam. |
|
Nto tas |
No.1, No.4, No.8 Daim iav tiav, 2b |
SA 240 GR 321 PHAJ TSHUAJ LAG LUAM
|
SS Qib |
C |
Si |
Mn |
P |
S |
Cr |
Mo |
Ni |
N |
Lwm |
|
|
Hom 321 |
min. |
- |
00.75 |
2.00 |
00.045 |
00.030 |
17.0 |
- |
9.0 |
00.10 |
Ti {=5 (c + n) |
Stainless hlau 321 phaj tshuab tej khoom
|
Ss hom |
Lub zog tensile yam tsawg kawg nkaus (MPA) |
Tos lub zog 0. 2% pov thawj yam tsawg (MPA) |
Elongation yam tsawg kawg (% hauv 50 hli) |
Kev nyuaj |
|
|
Rockwell B (HR B) Ntau |
Brinell (HB) siab kawg |
||||
|
321 |
515 |
205 |
40 |
95 |
217 |
SS 321 PHAJ Sib Xws Qib
|
Lub hom phiaj |
Werkstoff NR. |
Tsis yog |
JIS |
En |
|
321 |
1.4541 |
S32100 |
Sus321 |
X6cniti 18-10 |
ASTM A 240 321}} stainless hlau phaj ntawv thov
Khoom Siv Hluav Taws Xob
Tus sawv cev ua tub rog
Tshuaj Yeeb Nkab Vessels
Kev Tsim Kho
Kev Lag Luam Automotive
Cov Hluav Taws Xob Tshav Kub Kub
Conveyors
Khoom noj khoom haus ua thiab tuav