Stainless hlau Scrap Recycling: Yuav ua li cas cov khoom seem cuam tshuam rau tus nqi raw khoom

Jul 27, 2026

Tso lus

60-70% ntawm stainless hlau ntau lawm siv cov khoom siv rov ua dua tshiab raws li cov tswv yim tseem ceeb

 

Thaum koj yuavstainless hlau phaj, yeeb nkab, los yog bar, koj tsis yog them nyiaj nkauj xwb los ntawm kuv. Koj tab tom them nyiaj rau kev sib xyaw ua ke ntawm cov khoom siv rov ua dua tshiab, ferroalloys, thiab cov hlau tseem ceeb - thiab cov seem feem ntau dominates tus nqi qauv. Rau npib tsib xee- muaj cov qib xws li 304, 316, thiab npib tsib xee alloys, cov nqi seem uas nyob rau hauv cov khoom kawg tuaj yeem tshaj 40% ntawm tus nqi raw khoom.

 

Stainless Steel Scrap Recycling

 

Txawm li cas los xij feem ntau pawg neeg yuav khoom thiab cov engineers tsis tshua nug: Dab tsi yog tus nqi seem ntawm cov khoom kuv yuav? Tus nqi npib tsib xee cuam tshuam li cas tus nqi seem? Vim li cas 316 seem hais kom tus nqi tshaj 304? Kev nkag siab txog cov lus nug no ua rau koj muaj zog hauv kev sib tham, kev nkag siab txog tus nqi volatility, thiab ib daim duab meej dua ntawm kev txhawb nqa kev thov tom qab koj cov khoom.

 

Kev pom tseem ceeb: Stainless hlau seem tsis yog cov khoom pov tseg - nws yog qhov siab - tus nqi thib ob raw khoom uas nws tus nqi cuam tshuam ncaj qha rau koj lub mills alloy surcharge.

 

Kab lus no piav qhia txog yuav ua li cas stainless hlau seem rov ua haujlwm, cov nqi seem cuam tshuam li cas nrog LME npib tsib xee thiab chromium, thiab cov neeg yuav khoom yuav tsum paub dab tsi txog cov ntsiab lus siv dua tshiab hauv lawv cov ntaub ntawv pov thawj.

 

Dab tsi yog Stainless Hlau Scrap? Qib, Qhov Chaw, thiab Classification

 

Stainless hlau seem yog categorized los ntawm alloy cov ntsiab lus, daim ntawv, thiab huv si. Qhov siab dua cov nickel thiab molybdenum cov ntsiab lus, qhov muaj txiaj ntsig ntau dua cov seem - vim tias cov ntsiab lus alloying yog thawj tus nqi tsav tsheb hauv stainless hlau ntau lawm.

 

Thawj cov qhab nias thiab cov ntsiab lus nickel raug

 

Qhwv qib

Kev sib xyaw ua ke

Cov ntsiab lus (%)

Kwv yees li. Tus nqi ntau (USD / lb)

304 Sib

Cr 18-20%, Ni 8-10%

8-10%

$0.15-0.25

316 Sib

Cr 16-18%, Ni 10-14%, Mo 2-3%

10-14%

$0.30-0.45

Mixed Stainless

Ntau yam austenitic

4-12%

$0.20-0.35

Nickel Alloy (Inconel, Hastelloy)

Ni >50%, Cr, Mo, W, Co

50-60%+

$2.50-6.00+

400 Series (Ferritic / Martensitic)

Cr 11-17%, Tsis muaj Ni los yog tsawg Ni

0-2%

$0.08-0.12

Hloov / tho txawv

Machining pov tseg, mix

Hloov pauv

$0.10-0.20

 

Qhov chaw ntawm stainless hlau seem

 

Cov khoom siv hluav taws xob: Txiav- tawm, txiav, thiab tsis lees paub los ntawm cov khw muag khoom, cov yeeb nkab mills, thiab cov txheej txheem phaj. Ntxuav, zoo- yam ntxwv, tus nqi siab tshaj.

 

Cov khoom siv tsis siv neeg: Xaus- ntawm- cov khoom siv lub neej - cov khoom siv hauv chav ua noj, cov tso tsheb hlau luam, cov chaw tawm sab nrauv, cov khoom siv hluav taws xob. Yuav tsum tau sorting thiab tsom xam.

 

Cov khoom siv tam sim no: Tsim nyob rau hauv lub zeb nws tus kheej thaum dov, forging, los yog kev kho cua sov. Feem ntau rov qab ncaj qha mus rau qhov cub.

 

Nickel alloy scraps: Tawm - txiav los ntawm Inconel, Hastelloy, thiab Monel fabrication. Cov ntsiab lus nickel siab ua rau nws muaj nuj nqis heev - feem ntau muag rov qab rau cov neeg tsim khoom tshwj xeeb alloy.

 

316 stainless seem commands tus nqi 50-100% nqi tshaj 304 seem vim nws cov ntsiab lus molybdenum (2-3%) thiab ntau dua nickel (10-14%). Mo ib leeg tuaj yeem tsim nyog $ 15-25 ib kg ntawm cov hlau muaj.

 

Yuav ua li cas Stainless Hlau Scrap Recycled - EAF vs. AOD txheej txheem

 

Feem ntau stainless hlau niaj hnub no yog tsim nyob rau hauv Electric Arc Furnaces (EAF) siv ib tug siab feem pua ​​ntawm cov seem. Cov seem yog melted nrog ferrochromium, ferronickel, thiab lwm yam alloys, ces refined nyob rau hauv ib tug Argon -Oxygen Decarburization (AOD) lub nkoj kom ua tiav cov chemistry thiab cov ntsiab lus carbon tsawg.

 

How Stainless Steel Scrap Is Recycled

 

Cov txheej txheem rov ua dua hauv 5 kauj ruam

 

1. Kev Sau & Sorting: Cov khoom seem yog sau los ntawm cov chaw tsim khoom thiab txheeb xyuas qib uas siv cov khoom siv tes tuav XRF (PMI). Mixed loads raug muab cais ua 304, 316, 400-series, thiab lwm yam.

 

2. Kev Tshawb Fawb & Kev Ntsuam Xyuas: Cov qauv raug coj mus kuaj tshuaj. Cov khoom paug (tooj liab, txhuas, tin) raug txheeb xyuas thiab tshem tawm - lawv tuaj yeem ua rau kub luv lossis cuam tshuam rau cov khoom siv kho tshuab.

 

3. Them EAF: Cov khoom seem (50-80% ntawm tus nqi) yog thauj mus rau hauv lub tshuab hluav taws xob arc rauv nrog ferrochromium thiab ferronickel. Electrodes yaj qhov sib tov ntawm ~ 1600-1800 degree.

 

4. AOD Refining: Cov hlau molten raug xa mus rau AOD converter, qhov twg argon thiab oxygen tshuab los ntawm kev txo cov ntsiab lus carbon thiab kho cov qib Cr/Ni/Mo.

 

5. Casting & Rolling: Cov hlau tsis huv yog cam khwb cia rau hauv slabs, paj, los yog billets, ces kub - dov thiab txias - dov mus rau cov khoom kawg.

 

Vim li cas EAF + seem yog txoj kev tsim khoom tseem ceeb

 

Lub tshuab hluav taws xob arc rauv siv cov khoom seem yog lub zog ntau dua -nqi thiab qis dua -carbon dua li qhov cub tawg ua cov hlau tsis huv los ntawm ore. Rau cov hlau tsis muaj steel, txoj kev EAF feem ntau siv 50-70% tsawg zog thiab tso tawm 40-60% tsawg CO₂ ib tonne ntawm cov khoom tiav.

 

Txoj kev tsim khoom

Cov ntaub ntawv pov thawj (%)

Kev siv zog (GJ / t)

CO₂ Emissions (t / t)

Stainless hlau (EAF)

50-80%

8-12

0.8-1.5

Blast Furnace + BOF

10-25%

18-22

1.8-2.5

Integrated zeb (ore-raws li)

<15%

20-25

2.0-3.0

 

Sustainability ceeb toom: Siv 1 tonne ntawm stainless hlau seem txuag kwv yees li 1.5 tonnes ntawm hlau ore, 0.5 tonnes ntawm thee, thiab 1.2 tonnes ntawm CO₂ emissions piv rau cov nkauj xwb.

 

Yuav Ua Li Cas Khaub Ncaws Cov Nqi Sib Txuas Nrog LME Nickel thiab Alloy Surcharges

 

Stainless hlau seem nqi tsis teem nyob rau hauv kev sib cais. Lawv taug qab London Hlau Txauv (LME) nickel nqi, chromium ore nqi, thiab molybdenum oxide nqi - vim tias cov khoom seem yog los ntawm cov khoom alloying nws muaj.

 

Cov npib tsib xee- cov nqi sib txuas

 

304 stainless seem feem ntau muaj 8-10% npib tsib xee. Thaum LME npib tsib xee nce ntawm $ 12,000 / t txog $ 18,000 / t, tus nqi npib tsib xee hauv 304 seem nce 50%. Cov neeg muag khoom khib nyiab kho lawv cov nqi yuav khoom raws li, txawm tias nrog 2-4 lub lis piam lag.

 

Formula rau seem npib tsib xee tus nqi (simplified):

 

Nickel tus nqi hauv 304 seem=(Ni%) × (LME Ni nqe hauv $ / lb) × (rov qab zoo ~ 0.95). Piv txwv li: 9% Ni × $9.00/lb LME × 0.95=$0.77/lb nickel tus nqi hauv seem. Ntxiv tus nqi chromium (~ $ 0.15-0.20 / lb) thiab tus nqi hlau (~ $ 0.05-0.08 / lb) kom tau txais kwv yees tus nqi seem.

 

Kev sib txheeb keeb kwm: LME nickel vs . 304 seem (2020-2025)

 

Xyoo

LME Ni Avg ($/t)

304 Scrap Avg ($/t)

Kev sib txheeb

2020

$13,800

$1,100-1,400

Siab

2021

$18,400

$1,400-1,800

Siab heev

2022

$24,200

$1,800-2,400

Siab heev

2023

$20,500

$1,500-2,000

Siab

2024

$17,200

$1,200-1,700

Siab

2025 (TSI)

$15,800

$1,100-1,500

Siab

 

Vim li cas kev sib raug zoo tsis yog 100%

 

Cov khoom siv khib nyiab: Txawm tias tus nqi npib tsib xee nce, cov khoom seem yuav tsis muaj tam sim ntawd. Kev sau, txheeb xyuas, thiab logistics siv sijhawm.

 

Mill xav tau cov khoom seem: Yog tias qhov kev thov tsis muaj zog, mills txo cov khoom seem txawm tias npib tsib xee siab. Cov khib nyiab dhau los ua tus neeg yuav khoom lag luam.

 

Kev sib txawv hauv cheeb tsam: European thiab Asmeskas cov khw muag khoom seem ua raws li kev thov hauv zos thiab cov cai. Kev lag luam Asian (Tuam Tshoj, Is Nrias teb, Southeast Asia) muaj cov khoom siv sib txawv.

 

Alloy surcharge lag: Mills hloov kho alloy surcharge txhua hli. Cov nqi seem tuaj yeem txav tau txhua lub lim tiam. Qhov no tsim cov sijhawm luv luv - lub sijhawm arbitrage.

 

Yuav ua li cas Scrap tus nqi cuam tshuam hauv Alloy Surcharges

 

Thaum koj tau txais ib daim ntawv tsocai rau stainless hlau phaj lossis yeeb nkab, tus nqi feem ntau yog: Tus nqi pib (tso rau lub quarter) + Alloy surcharge (hloov kho txhua hli) + Kev them nyiaj ntxiv (yeem). Lub alloy surcharge yog qhov khoom seem ncaj qha cuam tshuam koj tus nqi.

 

How Scrap Value Is Reflected in Alloy Surcharges

 

Yuav ua li cas mills xam cov alloy surcharge

 

Kauj Ruam 1: Txiav txim siab cov ntsiab lus alloy - Rau 304, feem ntau 18% Cr, 9% Ni. Rau 316, ntxiv 2.5% Mo.

 

Kauj Ruam 2: Thov cov nqi raw khoom - Siv LME npib tsib xee, ferrochromium tus nqi, thiab molybdenum oxide nqi los ntawm hnub siv (feem ntau yog 15th ntawm lub hli dhau los).

 

Kauj Ruam 3: Tshem tawm cov nyiaj seem - Yog tias lub zeb siv 60% seem hauv tus nqi, lawv rov qab cov khoom seem uas muaj nqi. Qhov no txo ​​cov nqi ntxiv.

 

Kauj Ruam 4: Ntxiv cov nqi rov qab thiab cov nqi ua haujlwm - Kev poob thaum lub sij hawm melting, refining, thiab tuav yog suav nrog.

 

Piv txwv: 304 phaj alloy surcharge suav (simplified)

 

Cheebtsam

Kev suav

Tus nqi ($/t)

Cov ntsiab lus (9%)

$16,000/t Ni × 9%

$1,440

Cr cov ntsiab lus (18%)

$1.50/kg Cr × 18%

$270

Tsawg qhov credit (60%)

-$1,200/t seem × 60%

-$720

Kev ua & poob

5% ntawm tus nqi hlau

+$50

Tag nrho cov nqi ntxiv

Saum

$1,040/t

 

Kev pom zoo: Yog tias cov nqi seem poob sai dua li LME npib tsib xee, mills tuaj yeem ua rau lawv cov nyiaj seem thiab txo cov nqi ntxiv. Nug koj tus neeg muag khoom yuav ua li cas lawv cov qauv surcharge tswj cov nqi hloov pauv.

 

Nickel Alloy Scrap - Qhov siab tshaj plaws -Tus nqi rov siv dua hlau

 

Nickel alloy seem - Inconel, Hastelloy, Monel, Incoloy - yog nyob rau hauv ib pawg ntawm nws tus kheej. Nrog cov ntsiab lus npib tsib xee feem ntau tshaj 50%, thiab nrog molybdenum, chromium, cobalt, thiab tungsten kuj tam sim no, cov seem no tuaj yeem tsim nyog 5-20 × ntau dua li cov khoom seem.

 

Tus nqi nickel alloy qhov tseem ceeb (2025 kev ua lag luam)

 

Alloy

Nim Content

Lwm Yam Tseem Ceeb

Tus nqi seem ($/lb)

Ib 625

Ntau dua lossis sib npaug li 58%

Mo 8-10%, Cr 20-23%, Nb 3-4%

$4.00-6.00

Hastelloy C276

Ntau dua lossis sib npaug li 57%

Mo 15-17%, Cr 14-16%, W 3-4%

$5.00-7.00

Inconel 600

Ntau dua lossis sib npaug li 72%

Cr 14-17%

$3.50-5.00

Monel 400

Ntau dua lossis sib npaug li 63%

Kub 28-34%

$2.50-4.00

Incoloy 800 H

30-35%

Cr 19-23%, Fe tshuav nyiaj li cas

$1.00-2.00

 

Yog vim li cas nickel alloy seem muaj nuj nqis heev

 

High muaj nickel: Ntawm $ 16,000 / t nickel, 1 lb ntawm Inconel 625 seem muaj $ 0.90-1.00 ntawm nickel ib leeg.

 

Molybdenum thiab tungsten: Mo pauv ntawm $ 25-30 / kg, W ntawm $ 30-40 / kg. Hastelloy C276 seem tuaj yeem muaj $ 1.50-2.00 / lb ntawm Mo thiab W tus nqi.

 

Cobalt: Qee cov nickel alloys (xws li, Stellite, qee yam superalloys) muaj 5-20% Co, trading ntawm $ 30-40 / kg.

 

Kev ua lag luam tshwj xeeb: Tsuas yog ib txhais tes ntawm cov mills thoob ntiaj teb tuaj yeem ua cov nickel alloy seem. Cov mills no them tus nqi them rau cov khoom huv si, cais tawm.

 

Cov kev coj ua zoo tshaj plaws rau cov fabricators tuav cov nickel alloy seem

 

Segregate los ntawm qib: Tsis txhob sib xyaw Inconel 625 nrog Hastelloy C276. Txawm tias me me ntoo khaub lig- kis kab mob txo cov nqi seem los ntawm 20-40%.

 

Daim ntawv pov thawj cov ntaub ntawv pov thawj: Muab daim ntawv pov thawj zeb kuaj lossis PMI cov ntaub ntawv rau cov khoom seem. Txheeb xyuas cov khoom seem hais kom tus nqi siab dua.

 

Tsis txhob kis kab mob: Khaws cov tooj liab, txhuas, thiab lwm yam impurities tawm. Txawm tias 0.1% Cu tuaj yeem txo qis Hastelloy ntau.

 

Koom tes nrog cov neeg siv khoom tshwj xeeb: Cov khoom seem dav dav yuav tsis paub txog tus nqi tag nrho ntawm cov nickel alloys. Ua haujlwm nrog cov khoom siv rov ua dua tshiab uas tshwj xeeb hauv siab -temp thiab corrosion- tiv taus alloys.

 

Recycled Content Claims - Yuav Ua Li Cas Nug Koj Tus Muag Khoom

 

Ntau tus neeg muag khoom stainless hlau txhawb 「cov ntsiab lus rov ua dua tshiab」 raws li daim ntawv pov thawj kev ruaj ntseg. Tab sis qhov tseeb txhais li cas? Thiab koj tuaj yeem txheeb xyuas nws li cas?

 

Cov ntsiab lus rov siv dua qub thiab lawv txhais li cas tiag tiag

 

Thov

Nws txhais li cas

Kev Tshawb Fawb

Recycled cov ntsiab lus 60%

Cov khib nyiab ua 60% ntawm cov nqi hluav taws xob. Tej zaum muaj xws li sab hauv, industrial, thiab cov khoom siv tsis siv neeg.

Nug rau zeb qhov khoom seem ntawm cov khoom siv thiab xyoo. Xyuas EPD yog tias muaj.

Tshaj tawm - cov neeg siv khoom rov siv dua cov ntsiab lus

Cov khoom seem ntawm qhov kawg- ntawm- cov khoom siv lub neej (tsis muaj kev lag luam tawm- txiav). Nyuaj rau taug qab.

Thov cov ntaub ntawv pov thawj. Nrhiav rau thib peb- ntawv pov thawj tog.

100% recyclable

Cov khoom siv tuaj yeem rov ua dua thaum kawg ntawm lub neej - tab sis hais tsis muaj dab tsi txog cov ntsiab lus siv tam sim no.

Qhov no yog cov cuab yeej ntawm stainless hlau, tsis yog ib qho kev thov tshwj xeeb.

Carbon footprint 40% qis dua

Piv rau kev lag luam nruab nrab lossis ib qho kev ntsuas tshwj xeeb. Feem ntau xav tias EAF + kev ua haujlwm siab.

Tshawb xyuas EPD (Environmental Product Declaration) rau cov txheej txheem thiab kev ua haujlwm.

 

Yuav ua li cas txheeb xyuas cov ntsiab lus rov siv dua

 

Thov lub zeb qhov sib piv ntawm cov khoom seem: Nug qhov feem pua ​​​​ntawm cov khoom siv hauv cov khoom siv hluav taws xob rau cov khoom tshwj xeeb thiab lub sijhawm tsim khoom.

 

Nug rau EPD lossis LCA tsab ntawv ceeb toom: Environmental Product Declarations sau cov ntsiab lus rov siv dua thiab cov pa roj carbon hneev taw. Saib rau ISO 14025 lossis EN 15804 ua raws.

 

Tshawb xyuas -cov ntawv pov thawj thib peb: Qee lub mills tau ntawv pov thawj los ntawm cov koom haum xws li ISCC Plus lossis ResponsibleSteel, uas tshawb xyuas cov khoom seem thiab cov saw hlau- ntawm - saib xyuas.

 

Ceev faj ntawm cov lus tsis txaus ntseeg: 「Green steel」 lossis 「sustainable stainless」 yam tsis muaj ntaub ntawv yog kev lag luam, tsis yog pov thawj.

 

Lo lus nug tseem ceeb: Puas yog koj tus neeg muab khoom siv cov ntsiab lus rov qab hais txog cov nqi hluav taws xob (cov tswv yim) lossis cov khoom kawg (tso tawm)? Cov ntaub ntawv nkag mus siv tau yooj yim dua rau cov ntaub ntawv. Muab cov ntsiab lus rov ua dua tshiab yuav tsum muaj lub neej- kev tshuaj xyuas lub voj voog.

 

Stainless hlau khib Market Trends

 
Kev lag luam stainless hlau khib nyiab yog cuam tshuam los ntawm cov khoom siv nickel thoob ntiaj teb, Suav txoj cai tsim khoom, kev tswj hwm ib puag ncig, thiab kev xav tau los ntawm qhov kawg - siv cov haujlwm. Kev nkag siab txog cov qauv no yuav pab koj cia siab tias tus nqi txav mus los thiab npaj kev yuav khoom.
 
Stainless Steel Scrap Market Trends
 
Cov kev lag luam tseem ceeb hauv 2025-2026
 

LME nickel volatility: Nickel cov nqi tseem tsis hloov pauv vim Indonesia NPI (nickel npua hlau) nthuav dav, EV roj teeb xav tau, thiab kev lag luam speculative ntawm LME. Cov nqi seem ua raws nrog 2-4 lub lis piam lag.

 

Tuam Tshoj cov khoom siv khib nyiab: Tuam Tshoj yog lub ntiaj teb cov khoom lag luam stainless hlau loj tshaj plaws. Thaum Suav mills nce seem noj (tsav los ntawm ib puag ncig txoj cai lossis tus nqi), thoob ntiaj teb cov khoom seem nce.

 

EU CBAM cuam tshuam: Carbon ciam teb Kho Mechanism (CBAM) yuav nqi carbon emissions nyob rau hauv imported steel los ntawm 2026. Mills siv high-scrap, low-carbon txoj kev tau txais kev sib tw kom zoo dua.

 

Thib ob nickel mov: Nickel los ntawm cov khoom siv tsis zoo thiab cov roj teeb rov ua dua tshiab tau loj hlob. Qhov no tuaj yeem txo qis tus nqi npib tsib xee ntxiv rau lub sijhawm.

 

Cov khoom seem hauv cheeb tsam: Tebchaws Europe muaj cov txheej txheem sau cov khoom qub. Is Nrias teb thiab Southeast Asia tau nthuav dav sai. Middle East thiab Africa tseem tsis tau tsim kho.

 

Qhov twg mus taug qab stainless seem nqi

  • ScrapMonster (Tebchaws Asmeskas lag luam): Tracks 304, 316, thiab sib xyaw stainless seem nqi los ntawm cheeb tsam. Hloov tshiab ob-ib lub lim tiam.
  • Stainless Steel Club (ntiaj teb): Muab cov xov xwm kev lag luam niaj hnub, cov ntaub ntawv tus nqi, thiab kev tshuaj xyuas / kev xav tau rau 75 lub teb chaws.
  • Steel Nqe UK: Nyob UK cov nqi ib kg thiab ib tonne rau 304 thiab 316 stainless.
  • LME: Qhov siv rau nickel, chromium, thiab molybdenum nqi. Siv cov no kom nkag siab txog tus nqi alloy hauv seem.

 

Dab tsi stainless hlau cov neeg yuav khoom yuav tsum paub txog cov khoom seem

 

Raws li tus neeg yuav khoom ntawm cov khoom siv stainless hlau lossis npib tsib xee alloy, koj tsis tuaj yeem tuav cov khoom ncaj qha. Tab sis kev nkag siab txog tus nqi seem thiab rov ua dua tshiab ua rau koj muaj zog hauv kev sib tham thiab pab koj ntsuas cov neeg siv khoom thov.

 

What Stainless Steel Buyers Should Know About Scrap

 

5 nqe lus nug nug koj tus neeg muag khoom

 

Dab tsi yog koj lub zeb cov khoom siv khib nyiab rau cov khoom no? Nug seb qhov feem pua ​​​​ntawm cov khoom sib txawv thiab seb nws txawv ntawm cov khoom (plate vs. pipe vs. bar).

 

Yuav ua li cas koj lub alloy surcharge formula account rau seem nqi? Puas yog tus nqi ntxiv suav nrog cov credit? Qhov credit suav li cas?

 

Koj puas tuaj yeem muab EPD lossis LCA daim ntawv qhia txog cov ntaub ntawv siv dua tshiab? Saib rau ISO 14025 lossis EN 15804 ua raws. Tshawb xyuas cov haujlwm ua haujlwm thiab tshaj tawm cov ntsiab lus rov ua dua tshiab.

 

Lub hauv paus chiv keeb ntawm cov khoom siv yog dab tsi? Puas yog cov khoom seem hauv kev lag luam (them), cov khoom siv tsis siv neeg (post-cov neeg siv khoom), lossis cov khoom seem hauv tsev? Qhov no cuam tshuam rau kev thov nyiaj txiag ruaj khov.

 

Yuav ua li cas koj lis nickel alloy seem ntawm fabrication? Yog tias koj yog ib tus neeg tsim khoom ua haujlwm nrog Inconel lossis Hastelloy, nug seb lub zeb puas muaj cov kev pab cuam rov qab.

 

Yuav siv cov txuj ci seem li cas hauv kev sib tham

  1. Taug qab LME npib tsib xee thiab cov nqi seem: Yog tias npib tsib xee poob tab sis cov hlau tsis muaj nqi ntxiv, nug yog vim li cas. Lub zeb tej zaum yuav qeeb los hloov cov nyiaj seem.
  2. Sib piv cov qauv kev them nyiaj ntxiv: Qee lub mills siv cov nyiaj seem ruaj khov; lwm tus siv lub lag luam - txuas cov qauv. Cov tom kawg yuav yog pob tshab.
  3. Sib tham cov nqe lus yuav khoom rov qab: Yog tias koj tsim cov nickel alloy tseem ceeb, sib tham tus nqi yuav rov qab ua ntej. Qhov no tuaj yeem cuam tshuam koj cov nqi khoom siv los ntawm 5-15%.
  4. Sib tw vague sustainability claims: Nug cov ntaub ntawv. Ib tus neeg muag khoom uas tsis tuaj yeem muab EPD lossis cov ntaub ntawv pov tseg tuaj yeem tshaj tawm lawv cov ntsiab lus siv dua tshiab.

 

Cov lus nug nquag

 

Q: Vim li cas 316 stainless seem nqi ntau dua 304 seem?
A: 316 seem muaj molybdenum (2-3%), uas pauv ntawm $ 25-30 / kg - siab dua chromium. Mo ib leeg ntxiv $0.50-1.00/lb rau tus nqi seem. Ua ke nrog ntau dua npib tsib xee (10-14% vs . 8-10% hauv 304), 316 seem hais kom tus nqi 50-100%.

 

Q: Kuv puas tuaj yeem hais qhia cov ntsiab lus rov ua dua tshiab hauv kuv daim ntawv pov thawj khoom?
A: Feem ntau daim ntawv pov thawj zeb xeem (MTCs) tsis suav nrog cov ntsiab lus siv dua. Txawm li cas los xij, koj tuaj yeem thov Daim Ntawv Ceeb Toom Environmental Product Declaration (EPD) lossis ib tsab ntawv zeb hais txog qhov sib piv cov khoom seem. Qee lub mills muab ISCC Plus lossis ResponsibleSteel daim ntawv pov thawj rau cov ntaub ntawv rov ua dua tshiab.

 

Q: Ntau npaum li cas nickel rov qab los ntawm stainless hlau seem?
A: Hauv cov txheej txheem EAF + AOD niaj hnub, nickel rov qab los ntawm cov khoom seem tshaj 95%. Cov npib tsib xee tsis tau noj - nws tau rov-kua thiab dhau los ua ib feem ntawm cov hlau tsis huv tshiab. Qhov no yog vim li cas stainless hlau yog suav tias yog ib qho khoom siv 'mus tas li' hauv kev lag luam ncig.

 

Q: Puas yog cov hlau tsis zoo siv dua tshiab muaj cov khoom zoo ib yam li cov khoom siv nkauj xwb?
A: Yog. Thaum melted thiab refined, stainless hlau los ntawm seem yog chemically thiab mechanically zoo tib yam rau cov khoom ua los ntawm nkauj xwb ore. Cov txheej txheem AOD xyuas kom meej chemistry tswj tsis hais cov khoom nkag.

 

Q: Kuv yuav ua li cas nrog kuv cov nickel alloy seem ntawm fabrication?
A: Sib cais los ntawm qib thiab ua haujlwm nrog cov khoom siv tshwj xeeb uas ua haujlwm siab -nickel alloys. Sau cov seem nrog PMI tsom xam lossis daim ntawv pov thawj zeb. Kev huv, txheeb xyuas Inconel lossis Hastelloy seem tuaj yeem muag rau $ 3-7 / lb nyob ntawm qib thiab kev lag luam.

 

Q: Yuav ua li cas CBAM cuam tshuam tus nqi stainless hlau seem?
A: CBAM (Carbon ciam teb Kho Mechanism) yuav nqi cov pa roj carbon monoxide embedded nyob rau hauv imported steel. Mills siv siab -cov khib nyiab, EAF txoj kev muaj qis dua emissions thiab yuav raug nqi CBAM qis dua. Qhov no ua rau muaj kev xav tau ntawm cov khoom seem thiab tuaj yeem nce nqi seem txheeb ze rau nkauj xwb- khoom siv -raws li steel.

 

Q: Puas yog stainless hlau seem suav tias yog 'ntsuab' lossis ruaj khov?
A: Stainless hlau seem rov ua dua txo qis kev siv hluav taws xob, CO₂ emissions, thiab raw khoom extraction piv rau cov nkauj xwb. Txawm li cas los xij, 'ntsuab' daim ntawv thov yuav tsum tau txais kev txhawb nqa los ntawm LCA cov ntaub ntawv, tsis yog xav. Nrhiav EPDs thiab thib peb - ntawv pov thawj tog.

 

Xav tau Stainless Hlau lossis Nickel Alloy Cov Khoom Uas Muaj Kev Pom Zoo?

 

Ntawm jnalloy.com, peb muab stainless hlau thiab npib tsib xee alloy phaj, yeeb nkab, bar, thiab raj nrog tiav daim ntawv pov thawj zeb xeem (EN 10204 3.1/3.2), PMI pov thawj, thiab cov ntaub ntawv txhawb nqa. Peb ua haujlwm nrog cov mills siv siab - rov ua dua- cov ntsiab lus EAF txoj hauv kev thiab tuaj yeem muab cov ntaub ntawv EPD rau kev tshaj tawm kev ruaj ntseg.

 

Qib muaj: 304/304L, 316/316L, 321, 347, 904L, duplex S31803/S32750, Inconel 600/625, Hastelloy C276/C22, Incoloy 800H/825, thiab lwm yam.

Hu rau peb pab neeg muag khoom technical:

Email: Market@jnalloy.com

Xov tooj/WhatsApp: +86-193-3990-0211

Lub Vev Xaib: www.jnalloy.com

 

Xa kev nug
Los rau peb
Thiab pib koj rfqs tam sim no.
Tiv Tauj Peb