Stainless Hlau Phaj vs Sheet: Thickness, Standards, thiab Application Differences

Jul 02, 2026

Tso lus

Tshawb nrhiav qhov sib txawv tseem ceeb ntawmstainless hlau phaj thiab ntawv- thickness ciam teb (4.75 hli), ASTM A240/A480 tus qauv, nto tiav, thiab cov txheej txheem xaiv cov ntawv thov. Kawm seb daim ntawv twg haum rau koj qhov project.

 

Stainless Steel Plate vs Sheet

 

Qhov sib txawv ntawm stainless hlau phaj thiab daim ntawv yog thickness.Kev lag luam- tus qauv ciam teb yog3/16 nti (4.75mm): khoom ntawm los yog saum toj no thickness yog cais raws liphaj; dab tsi yog thinnerdaim ntawv. Qhov kev txiav tawm ib leeg no ua rau muaj qhov sib txawv ntawm txoj kev tsim khoom, muaj cov khoom tiav, qhov ntev ntev, thiab kawg - siv daim ntawv thov.

 

Metric

Tus nqi

Thickness ciam teb (phaj vs daim ntawv)

3/16 nti=4.75 hli (ASTM A480)

Cov khoom siv tseem ceeb

ASTM A240/A240M

Primary kam rau ua & xa tus qauv

ASTM A480 / A480M ASTM

Yam tsawg kawg ntawm daim ntawv dav

24 nti (610mm)

Yam tsawg kawg ntawm phaj dav

>10 nti (254 hli)

Hom ntawv thickness ntau yam

0.30-4.75 hli

Hom phaj thickness ntau yam

4.75mm - 200+ hli

Cov qib austenitic feem ntau

304/304L, 316/316L, 321

Cov qeb tshwj xeeb

17-4PH, Duplex 2205, Super Duplex 2507

Plate nto tiav (typical)

Tsis yog . 1 (Kub Rolled Annealed & Pickled)

Sheet nto finishes (zoo)

2B, BA (Zoo Annealed), Tsis yog. 4, Tsis yog. 8

 

Dab tsi yog qhov txawv ntawm Stainless Hlau Phaj thiab Sheet?

 

Thawj qhov sib txawv yog tuab: phaj yog 3/16 nti (4.75 hli) los yog tuab dua, thaum daim ntawv yog thinner dua 3/16 nti.Lub ciam teb no, tsim nyob rau hauv ASTM A480/A480M (Standard Specification for General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Phaj, Sheet, and Strip), yog ib qho tseem ceeb tshaj plaws uas cais ob hom khoom. Txawm li cas los xij, qhov txawv txav tau zoo tshaj li tus lej ntawm lub caliper - nws cascades rau hauv cov txheej txheem tsim khoom, cov kev xaiv ua tiav, cov kab siab ntev, cov qauv nqi, thiab kev tsim nyog rau cov ntawv thov tshwj xeeb.

 

Hauv cov ntsiab lus tswv yim, yog tias koj xaj khoom 3 hli tuab 304 stainless hlau tiaj tus, koj tab tom xajdaim ntawv. Yog tias koj xaj khoom 6 hli tuab 316L tiaj tus, koj tab tom xajphaj. Cov khoom siv chemistry yuav zoo ib yam, tab sis txoj kev tsim khoom, cov khoom siv kho tshuab, thiab cov khoom tiav yuav txawv.

 

Dab tsi yog Tus Txheej Txheem Thickness Ciam Teb?

 

Tus qauv thickness ciam nruab nrab ntawm stainless hlau phaj thiab daim ntawv yog 3/16 nti (4.75 mm), raws li tau hais nyob rau hauv ASTM A480 / A480M.Cov khoom siv nrog lub nominal thickness ntawm lossis siab dua 3/16 nti yog cais raws li phaj; cov ntaub ntawv hauv qab no yog cais raws li daim ntawv. Dav kuj tseem ua lub luag haujlwm hauv kev faib tawm: daim ntawv yuav tsum muaj qhov dav tsawg kawg nkaus ntawm 24 ntiv tes (610 hli), thaum phaj xav tau qhov dav ntau dua 10 ntiv tes (254 hli). Cov khoom me me hauv qab 3/16 nti yog cais raws li sawb.

 

What Is the Standard Thickness Boundary

 

Pav ca- Rolled Stainless Steel Product Classification

 

Yam khoom

Thickness Ntau

Yam tsawg kawg nkaus

Kev tswj hwm tus qauv

Ntawv nyiaj

Txog li 0.005 nti (0.13mm)

-

ASTM A240 / A480

Daim ntawv

0.30mm-4.75 hli

Ntau dua lossis sib npaug li 24 hauv (610 mm)

ASTM A240 / A480

Sawb

0.30mm-4.75 hli

< 24 in (610 mm)

ASTM A240 / A480

Phaj

Ntau dua lossis sib npaug li 4.75 hli (3/16 hauv)

>10 nyob rau hauv (254 mm)

ASTM A240 / A480

 

Kev nkag siab tseem ceeb:Lub 4.75 hli ciam teb tsis yog arbitrary. Hauv qab no cov tuab, cov khoom siv tuaj yeem ua tau zoo txias - dov kom ua tiav qhov ntev ntev thiab du nto tiav. Saum toj no cov tuab, txias dov yuav ua tsis tau raws li qhov yuav tsum tau ua, yog li kub dov ua thawj txoj kev tsim khoom - uas inherently ua rau rougher nto thiab dav ntev ntev bands.

 

Cov txheej txheem tsim khoom sib txawv li cas?

 

Cov hlau tsis muaj steel feem ntau yog kub- dov, thaum cov ntawv tuaj yeem kub - dov los yog txias - dov nyob ntawm lub hom phiaj thickness thiab nto tiav.Kub dov yuav hla cov hlau los ntawm cov yob ntawm qhov kub siab tshaj qhov recrystallization point (feem ntau 1100-1250℃rau stainless hlau). Qhov no tso cai rau txo qhov thickness ntawm ib zaug xwb tab sis ua rau scaly, tsaus nto uas yuav tsum tau muab annealed thiab pickled (Tsis yog . 1 tas). Txias dov, ua nyob rau hauv chav tsev kub, tsuas yog txo cov thickness nyob rau hauv me me increments tab sis ua tiav superior nto zoo, nruj tolerances, thiab siab zog los ntawm kev ua hauj lwm hardening.

 

Kev sib piv kev tsim khoom

Parameter

Phaj

Daim ntawv

Thawj txoj kev dov

Kub dov

Kub dov (thicker) los yog txias dov (thinner)

Hom kev tsim khoom

Kub yob → anneal → pickle → deg mob

Kub yob → anneal → pickle → txias yob → kawg anneal → pickle / tiav

Nto tom qab ntau lawm

Tsis yog . 1 (dub, ntxhib, pickled)

2B (zoo, grey, txias-khoov) lossis BA (ci)

Dimensional kam rau ua

Dav (± kam rau ua rau ASTM A480)

Tighter (± kam rau ua rau ASTM A480)

Ua hauj lwm hardening nyhuv

Yam tsawg kawg nkaus (annealed)

Qhov tseem ceeb rau txias - dov tempers (ib ASTM A666)

Hom max ib zaug - txo qis

Txog li 50% +

2-10% rau ib qho kev xeem

Tus nqi ib kg (ib qib)

Lower (tsawg dua cov kauj ruam ua)

Siab dua (qhov txias ntxiv- dov thiab ua tiav)

 

Rau tib qib - piv txwv li, 316L - 3 hli txias- dov daim ntawv feem ntau yuav muaj zog ntau dua li 6 hli kub- dov phaj nyob rau hauv qhov mob annealed, vim qhov txias - dov txheej txheem qhia ua hauj lwm hardening. Txawm li cas los xij, yog tias daim ntawv yog tom qab kev daws teeb meem-annealed, ob daim ntawv yuav pom cov khoom zoo sib xws, vim tias qhov annealing tshem tawm cov hauj lwm- cov nyhuv hardening thiab rov ua kom cov khoom mus rau nws lub xeev softened.

 

Dab tsi yog cov qauv tswj hwm stainless hlau phaj thiab ntawv?

 

ASTM A240 / A240M thiab ASTM A480 / A480M yog ob lub hauv paus qauv tswj hwm stainless hlau phaj thiab ntawv hauv Tebchaws Meskas.ASTM A240 txhais cov khoom siv dab tsiyog- nws cov tshuaj muaj pes tsawg leeg, txhua yam khoom, thiab cua sov- kev kho mob yuav tsum tau ua. ASTM A480 txhais cov khoom siv li casxa- qhov ntev kam rau ua, qhov chaw tiav, thiab cov ntaub ntawv xaj. Cov sib npaug thoob ntiaj teb muaj nyob hauv Europe (EN 10088), Nyiv (JIS G4304 / G4305), thiab Tuam Tshoj (GB / T 4237 / 4238).

 

What Standards Govern Stainless Steel Plate and Sheet

 

Cov qauv tseem ceeb rau cov khoom lag luam stainless hlau tiaj tus

Txuj

Scope

Yam Nws Tswj

ASTM A240/A240M

Phaj, ntawv, sawb rau cov hlab ntsha siab thiab kev siv dav dav

Chemistry, mechanical zog, kho cua sov, kuaj

ASTM A480 / A480M ASTM

Cov kev cai dav dav rau cov pav ca -rolled stainless

Thickness/dav tolerances, flatness, nto tiav, xaj info

ASTM A666 Cov khoom lag luam

Annealed los yog txias -ua haujlwm austenitic ntawv, sawb, phaj

Temper designations, mechanical properties for txias-ua hauj lwm tempers

ASME SA-240 / SA-480

ASTM A240 / A480 Cov Lus Qhia Tshwj Xeeb

Ib yam li ASTM cov neeg sib tw, tau lees paub rau ASME Boiler & Pressure Vessel Code

TS EN 10088-2

European stainless hlau ntawv / phaj / sawb

Chemistry, mechanical zog, nto finishes (European designations)

JIS G4304/G4305

Japanese kub- dov / txias- dov stainless phaj & ntawv

Chemistry, Mechanical Properties, Dimensions (Japanese qib)

GB/T 4237/GB/T 4238

Suav kub-rolled phaj / txias-rolled ntawv

Chemistry, txhua yam khoom, qhov ntev (Suav qib)

Practical takeaway:Thaum xaj cov khoom lag luam stainless hlau tiaj tus, koj yuav tsum qhia ob qho qauv - piv txwv li, "316L stainless hlau phaj, ASTM A240 / A480, Tsis yog. 1 tiav." Thawj ua kom cov khoom ua tau raws li chemistry thiab cov khoom yuav tsum tau ua; qhov thib ob ua kom nws ua tau raws li qhov yuav tsum tau muaj thiab qhov chaw koj xav tau.

 

Yuav Ua Li Cas Deg Finishes Sib Piv?

 

Cov phaj feem ntau muaj nyob rau hauv ntau yam kev ua tiav (feem ntau Tsis yog. 1), thaum cov ntawv muaj qhov dav dav los ntawm kev lag luam 2B mus rau daim iav- polished Tsis yog . 8.Qhov no yog qhov tshwm sim ncaj qha ntawm cov txheej txheem tsim khoom: kub- cov phaj dov muaj qhov ntxhib ntxhib, scaly nto uas tau ntxuav los ntawm annealing thiab pickling tab sis tsis ntxiv refined. Txias- cov ntawv dov, los ntawm qhov sib piv, tuaj yeem ua tiav los ntawm kev ua tiav ntxiv - sib tsoo, polishing, lossis buffing - kom ua tiav cov npoo zoo dua thiab muaj kev cuam tshuam ntau dua.

 

Surface Finish Availability los ntawm Cov Khoom Muag

 

Finish Designation

Kev piav qhia

Phaj

Daim ntawv

Tsis yog . 1

Kub- dov, annealed, pickled - tsaus, ntxhib

Yog (standard)

Yog (thicker gauges)

Tsis yog . 2D

Txias- dov, annealed, pickled - dull

Tsis muaj

Yog lawm

2B

Txias- dov, annealed, pickled, tawv nqaij- dhau - du, grey

Tsis muaj

Yog (feem ntau)

BA (Zoo Annealed)

Txias- dov, ci annealed - reflective

Tsis muaj

Yog lawm

Tsis yog . 4 (Txhim kho)

Mechanically polished nrog abrasive - directional grain

Ua tau (kev txiav txim tshwj xeeb)

Yog lawm

Tsis yog . 6

Tampico txhuam - duller dua No. 4

Tsis muaj

Yog (kev txiav txim tshwj xeeb)

Tsis yog . 7 (Reflective)

Buffed - ib nrab -reflective

Tsis muaj

Yog (kev txiav txim tshwj xeeb)

Tsis yog . 8 (Daim iav)

Buffed rau daim iav tiav - muaj kev cuam tshuam heev

Tsis muaj

Yog (kev txiav txim tshwj xeeb)

 

Daim ntawv thov:Yog tias koj qhov project yuav tsum tau ua kom zoo nkauj lossis huv si - piv txwv li, zaub mov - cov khoom siv ua haujlwm, chav tsev tshuaj huv huv, lossis cov khoom siv vaj tsev zoo nkauj -, koj yuav luag xav tau cov ntaub ntawv nrog 2B, Tsis yog . 4, lossis BA tiav. Daim hlau tsis muaj. 1 tiav yog tsim nyog rau cov qauv, siab- muaj, lossis zais daim ntawv thov uas qhov kev zoo nkauj ntawm qhov chaw tsis tseem ceeb.

 

Daim ntawv thov sib txawv yog dab tsi?

 

Cov phaj raug xaiv rau lub zog ntawm cov qauv, kev ntim siab, thiab hnyav- kev pabcuam kev lag luam; cov ntawv yog xaiv rau formability, deg aesthetics, thiab siv lub teeb yuag.Lub thickness sib txawv ncaj qha dictates dab tsi txhua daim ntawv yuav ua tau. Phaj muab cov phab ntsa tuab uas xav tau los tiv thaiv lub siab sab hauv hauv cov hlab ntsha, nqa cov khoom siv hauv cov txuas hniav thiab cov platforms, thiab tiv thaiv kev yaig hauv kev ua tshuaj lom neeg. Cov nplooj ntawv muab qhov nyias, tsim tau, thiab zoo nkauj zoo nkauj qhov chaw uas xav tau rau cov neeg siv khoom -ntsig thiab huv si- cov ntawv thov tseem ceeb.

 

Daim ntawv thov sib piv los ntawm Kev Lag Luam

 

Kev lag luam / Daim Ntawv Thov

Hom ntawv

Vim li cas daim ntawv no raug xaiv

Siab hlab ntsha & boilers

Phaj

Thickness xav tau rau lub siab ntim ib ASME Code

Kub exchangers (tubesheets)

Phaj

Thickness xav tau rau raj - mus rau -tubesheet kev sib koom ua ke

Cov qauv kab teeb & platforms

Phaj

Load- bearing muaj peev xwm yuav tsum thickness > 5 mm

Chemical & petrochemical tanks

Phaj

Corrosion nyiaj pub + kev ruaj ntseg ntawm cov thickness

Marine & offshore

Phaj

Thick seem rau hulls, bulkheads, thiab structural cov tswv cuab

Nuclear & zog tsim

Phaj

Cov ntu tuab rau cov hlab ntsha reactor thiab cov tshuab hluav taws xob

Cov khoom siv ua zaub mov

Daim ntawv

Nyias, formable, huv si 2B/No. 4 nto; yooj yim rau vuam thiab ntxuav

Pharmaceutical huv chav

Daim ntawv

Smooth BA los yog Tsis muaj . 4 ua kom tiav rau kev huv thiab kev tswj kev sib kis

Architectural cladding & facades

Daim ntawv

Aesthetic tiav (Tsis yog. 4, BA, Tsis yog. 8); lub teeb yuag panels

Cov khoom siv hauv chav ua noj & dab dej

Daim ntawv

Sib sib zog nqus- kos duab formability; ci, zoo nkauj nto

Automotive trim & tso pa tawm

Daim ntawv

Nyias ntsuas, formable, weldable rau complex duab

Cov cuab yeej kho mob & cov tais

Daim ntawv

Nyias, meej, sterilizable nto

 

Yuav Ua Li Cas Tolerances thiab Dimensional Accuracy Sib Piv?

 

Cov nplooj ntawv - tshwj xeeb txias- cov ntawv dov - muaj cov tuab tuab tuab dua li cov phaj, vim tias txias dov muab cov tuab tuab ntau dua li cov dov kub.ASTM A480/A480M txhais cov lus sib cais rau cov kub- dov phaj, kub- dov daim ntawv / sawb, thiab txias- dov daim ntawv / sawb. Raws li txoj cai dav dav, txias-rolled sheet tolerances yog kwv yees li 40-60% nruj dua kub-rolled phaj kam rau ntawm qhov sib piv nominal thicknesses. Qhov sib txawv no yog qhov tseem ceeb rau cov ntawv thov uas xav tau kev sib haum xeeb- nce hauv vuam, machining nyiaj pub dawb, lossis kev sib hloov ntawm qhov chaw.

 

How Do Tolerances and Dimensional Accuracy Compare

 

Kev sib piv kam rau siab (Ib qho piv txwv, rau ASTM A480)

 

Nominal Thickness

Kub-Rolled Phaj Tolerance

Txias -Rolled Sheet Tolerance

Kev txhim kho Factor

3 hli (0.118 nti)

± 0.20 hli

± 0.08 hli

2.5 × qhov siab

5 hli (0.197 nti)

± 0.25 hli

± 0.10 hli

2.5 × qhov siab

8 hli (0.315 nti)

± 0.30 hli

- (feem ntau yog HR nkaus xwb)

N/A

12 hli (0.472 nti)

± 0.35 hli

-

N/A

20 hli (0.787 nti)

± 0.40 hli

-

N/A

Lus Cim: Qhov tseeb qhov siab ntev sib txawv ntawm qhov dav thiab cov lus tshwj xeeb ASTM A480. Nco ntsoov sab laj tus qauv tam sim no rau cov lej tseeb uas siv tau rau koj qhov kev txiav txim qhov ntev.

 

Flatness kam rau uakuj txawv. Cov phaj yog ua raws li kev ua siab ntev ntev teev hauv ASTM A480, uas tso cai rau qee qhov sib txawv ntawm ib chav tsev ntawm qhov dav. Cov ntawv, ua nyias thiab hloov tau yooj yim, feem ntau yog muab rau hauv daim ntawv tiaj tus lossis coil thiab tsis tuav rau tib lub phaj flatness. Rau cov ntawv thov uas yuav tsum tau tshwj xeeb flatness (xws li, precision tooling los yog kho qhov muag khoom), ntxiv flattening hauj lwm xws li stretcher leveling los yog roller leveling tej zaum yuav tsim nyog.

 

Phaj vs Sheet: Yam Koj Yuav Tsum Xaiv?

 

Xaiv cov phaj thaum muaj kev ncaj ncees, kev tswj hwm, lossis kev tiv thaiv corrosion xav tau thickness. Xaiv daim ntawv thaum formability, nto tiav, txo qhov hnyav, los yog tus nqi efficiency ntawm nyias gauges yog qhov tseem ceeb.Qhov kev txiav txim siab yuav tsum tau tsav los ntawm daim ntawv thov yuav tsum tau - tsis yog los ntawm qhov muaj lossis tus cwj pwm. Hauv qab no yog lub tswv yim kev txiav txim siab los coj koj xaiv.

 

Kev txiav txim Factor

Xaiv Phaj Yog...

Xaiv Daim Ntawv Yog...

Tsim siab / load

Siab siab los yog hnyav structural load

Tsawg lossis tsis muaj siab; tsis yog - qauv

Yuav tsum tau thickness

Ntau dua lossis sib npaug li 4.75 hli (3/16 hauv)

< 4.75 mm (3/16 in)

Qhov yuav tsum tau ua kom tiav

Tsis muaj . 1 (kev lag luam) txais tau

2B, BA, Tsis yog . 4, lossis Tsis yog . 8 tiav lawm

Tsim / sib sib zog nqus kos duab

Txwv kev tsim; feem ntau yog txiav / vuam

Kev nthuav dav, khoov, lossis kos duab sib sib zog nqus

Qhov hnyav rhiab heev

Qhov hnyav tsis yog thawj qhov kev txhawj xeeb

Kev txo qhov hnyav yog qhov tseem ceeb (piv txwv li, thauj, aerospace)

Vuam txoj kev

Thick -section welding (ntau-pass)

Nyias-gauge vuam (ib zaug-pass, TIG/laser)

Corrosion pub

Cov nyiaj pab tseem ceeb uas xav tau tshaj lub neej ua haujlwm

Yam tsawg kawg nkaus; kev tiv thaiv nto txaus

Tus nqi rhiab heev (ib kg)

Tus nqi qis dua ib kg nyiam

Tus nqi siab dua ib kg txais tau rau kev ua tiav / formability

Kev cai ua raws cai

ASME Boiler & Pressure Vessel Code

FDA, zaub mov- qib, lossis cov qauv kev tu cev

 

Hom Stainless Hlau Qib Muaj nyob rau hauv ob daim ntawv

 

Feem ntau cov austenitic, duplex, thiab nag lossis daus- cov qib stainless hlau hardening muaj nyob rau hauv ob daim ntawv phaj thiab daim ntawv, txawm tias muaj sib txawv los ntawm thickness thiab qib ua ke.Cov lus hauv qab no qhia txog cov qib uas feem ntau teev tseg rau cov khoom tiaj tus, lawv cov yam ntxwv tseem ceeb, thiab muaj nyob hauv txhua daim ntawv.

 

Qib Muaj thiab yam ntxwv

Qib (UNS)

Hom

Cov yam ntxwv tseem ceeb

Phaj

Daim ntawv

304 / 304L (S30400/S30403)

Austenitic

General -lub hom phiaj; zoo heev weldability thiab formability

Yog lawm

Yog lawm

316 / 316L (S31600/S31603)

Austenitic

Ntxiv Mo rau pitting kuj; marine & tshuaj

Yog lawm

Yog lawm

321 (S32100)

Austenitic

Ti-stabilized rau qhov kub thiab txias

Yog lawm

Yog lawm

309S / 310S (S30908/S31008)

Austenitic

High Cr / Ni rau oxidation tsis kam mus rau 1100 degree

Yog lawm

txwv

17-4PH (S17400)

Cov nag lossis daus Hardening

Lub zog siab + zoo corrosion kuj; hnub nyoog- nyuaj

Yog lawm

Yog lawm

Duplex 2205 (S32205)

Duplex

2 × yield zog ntawm 316L; Zoo heev chloride SCC kuj

Yog lawm

Yog lawm

Super Duplex 2507 (S32750)

Super Duplex

Maximum corrosion kuj; rau kev pabcuam chloride hnyav

Yog lawm

txwv

904L (N08904)

Austenitic

High - alloy rau sulfuric acid thiab chloride ib puag ncig

Yog lawm

Yog lawm

 

Cov lus nug nquag

 
Q1: Puas muaj qhov sib txawv ntawm cov tshuaj muaj pes tsawg leeg ntawm cov phaj thiab cov ntawv ntawm tib qib?

Tsis muaj.Yog tias ob lub phaj thiab daim ntawv tau lees paub rau tib qib kev xaiv (piv txwv li, 316L ib ASTM A240), lawv cov kev xav tau tshuaj muaj pes tsawg leeg zoo ib yam. Qib specification hauv ASTM A240 tsis txawv ntawm cov khoom siv - ib daim ntawv 3 hli thiab 20 hli phaj ntawm 316L ob leeg yuav tsum tau raws li tib chemistry txwv rau carbon, chromium, nickel, molybdenum, thiab lwm yam khoom.

 

Q2: Stainless hlau phaj puas tuaj yeem txias - dov?

Feem ntau, tsis muaj - tsis nyob ntawm qhov tuab tuab.Txias dov yog qhov ua tau zoo rau cov khoom siv txog li 4-5 hli hauv thickness. Saum toj no, lub dov quab yuam yuav tsum tshaj qhov txias- dov mills tuaj yeem xa khoom lag luam. Qee lub phaj yuav tau txais lub teeb txias- dov dhau (dawb daim tawv nqaij- dhau) txhawm rau txhim kho flatness lossis nto, tab sis qhov no tsis yog qhov txias txias. Rau cov phaj nyias nyob ze ntawm 4.75 mm ciam teb, cov mills tshwj xeeb tuaj yeem muab cov kev xaiv txias -rolled, tab sis kub dov tseem yog cov qauv tsim rau phaj.

 

Q3: Dab tsi yog qhov txawv ntawm 2B thiab BA nto tiav?

2B yog khaub thuas- dov, annealed, pickled, thiab daim tawv nqaij- dhau tag nrog ib tug du tab sis tsis yog - reflective grey nto.BA (Bright Annealed) yog txias - dov thiab annealed nyob rau hauv ib tug tswj hydrogen cua, ua ib tug kaj, reflective nto tsis muaj mechanical polishing. BA yog smoother thiab muaj kev cuam tshuam ntau dua li 2B tab sis feem ntau kim dua thiab muaj nyob rau hauv cov ntsuas nyias. Ob leeg yog daim ntawv- tsuas yog tiav; lawv tsis muaj nyob rau ntawm kub -rolled phaj.

 

Q4: Vim li cas phaj feem ntau pheej yig dua ib kilogram dua li daim ntawv ntawm tib qib?

Vim tias phaj yuav tsum tau ua cov kauj ruam tsawg dua.Phaj yog kub- dov, annealed, thiab pickled - feem ntau yog peb txoj haujlwm loj. Daim ntawv (txias-dov) mus los ntawm kub dov, annealing, pickling,cestxias dov, qhov thib ob annealing, thiab zaum kawg pickling lossis tiav - tsib los yog ntau tshaj kev ua haujlwm. Txhua kauj ruam ntxiv ntxiv cov nqi zog, lub zog, thiab cov khoom siv. Tsis tas li ntawd, cov ntawv txias -rolled feem ntau muaj nruj dua kev ua haujlwm siab thiab siab dua qhov zoo, uas ua rau tus nqi hwm.

 

Q5: Kuv puas tuaj yeem siv daim ntawv hloov phaj kom txuag tau nqi?

Tsuas yog tus tsim tso cai rau nws.Yog tias daim ntawv thov yuav tsum muaj qhov tsawg kawg nkaus thickness rau lub siab ntim, cov qauv thauj khoom, lossis kev tiv thaiv corrosion, hloov cov ntawv nyias nyias rau phaj yuav cuam tshuam kev nyab xeeb thiab kev ua raws cai. Txawm li cas los xij, yog tias tus qauv tsim yog tuab- yoog raws (piv txwv li, ib qho tsis yog - cov ntaub thaiv npog los yog liner), siv cov ntawv nyias nyias nyias - cov ntawv yob tuaj yeem txo cov khoom hnyav thiab tus nqi. Nco ntsoov sab laj nrog tus kws tsim khoom tsim nyog ua ntej hloov cov ntaub ntawv khoom hauv daim ntawv thov kev tswj hwm.

 

Q6: Qhov txawv ntawm ASTM A240 thiab ASME SA-240 yog dab tsi?

ASME SA-240 yog Boiler thiab Pressure Vessel Code txais yuav ntawm ASTM A240.Cov txheej txheem kev cai yog qhov tseem ceeb zoo ib yam. Qhov sib txawv tseem ceeb yog daim ntawv pov thawj: cov ntaub ntawv pov thawj rau ASME SA-240 yog siv tau rau hauv cov hlab ntsha siab uas tsim nyob rau hauv ASME Code, nrog rau tag nrho traceability thiab cov ntaub ntawv pov thawj (Cov ntaub ntawv xeem ntawm EN 10204 3.1 lossis 3.2). Rau cov ntawv thov tsis muaj zog, ASTM A240 ntawv pov thawj feem ntau txaus.

 