Duplex stainless hlau 2205 phaj, tseem hu ua S32205 lossis 2205 duplex phaj, muaj lub zog siab thiab zoo heev corrosion kuj ntawm tus nqi tsim nyog. Engineers xaiv nws thaum 316L stainless hlau tsis muaj zog txaus tab sis super duplex S32750 yog kim heev.

Ntawm peb lub Hoobkas tsim tshwj xeeb hauv cov khoom siv stainless hlau thiab npib tsib xee alloy, peb tsim S32205 daim hlau txhua hnub rau ASTM A240 thiab ASME SA240 cov qauv. Hauv tsab xov xwm no, peb muab cov lus qhia meej 2026 tus nqi ntawm duplex 2205 phaj.
Tam sim no Duplex 2205 Phaj Nqe Ib Kg
Qhov nruab nrab 2205 duplex stainless hlau phaj nqi ib kg hnub no yog li ntawm $ 4.80 txog $ 7.20, nyob ntawm thickness, ntau, thiab qib ntawv pov thawj. Peb lub Hoobkas- tus nqi ncaj qha feem ntau yog 15-25% qis dua tus nqi xa tawm vim tias peb yaj, yob, thiab sim cov khoom peb tus kheej.
Table 1: Duplex 2205 Phaj Nqe Ib Kg los ntawm Thickness (FOB Tuam Tshoj, USD / kg)
|
Thickness (hli) |
Tus nqi ntau (USD / kg) |
Nqe rau 1-5 tons |
Nqe rau 10+ tons |
Daim ntawv thov |
|
3–6 |
6.20 – 7.20 |
6.80 |
6.20 |
Linings, cladding, me me hlab ntsha |
|
8–12 |
5.60 – 6.50 |
6.10 |
5.60 |
Tank, kub exchangers |
|
15–20 |
5.10 – 5.90 |
5.60 |
5.10 |
Cov hlab ntsha siab, platforms |
|
25–30 |
4.90 – 5.60 |
5.30 |
4.90 |
Cov qauv hauv paus, hnyav piping |
|
40–50 |
5.00 – 5.80 |
5.40 |
5.00 |
High -siab reactors |
Cov nqi no suav nrog Kev Ntsuas Cov Khoom Siv Zoo, kev tshuaj xyuas ultrasonic, thiab daim ntawv pov thawj tag nrho cov ntawv pov thawj zeb. Rau PED lossis NORSOK daim ntawv pov thawj, ntxiv $0.30–$0.50 ib kg. Tag nrho cov nqi yog rau 2B lossis No.1 tiav; iav polish los yog kev cai beveling ntxiv $0.40–$0.80 ib kg.
Nqe los ntawm Quantity thiab Order Size
Kev yuav ntau txuag nyiaj. Kev txiav txim me me (hauv qab 500 kg) raug nqi siab tshaj tus nqi ib kg. Kev txiav txim 10-tuj tuaj yeem txo qhov duplex 2205 phaj nqi ib kg txog li 18%. Peb kuj muab daim ntawv cog lus rau cov khoom txhua xyoo uas kaw cov nqi thiab tiv thaiv koj ntawm kev ua lag luam txhua hli.
Dab tsi cuam tshuam rau Duplex 2205 Phaj Nqe Ib Kg?

Plaub yam tseem ceeb tswj tus nqi kawg:
Cov nqi raw khoom
Nickel, molybdenum, thiab nitrogen nqi hloov txhua lub lim tiam. Hauv 2026, npib tsib xee nruab nrab yog $ 18,000 ib tuj. Thaum npib tsib xee nce $1,000 ib tuj, 2205 phaj nqi ib kg nce txog $0.15.
Phaj Thickness thiab Loj
Cov phaj nyias nyias (3-6 hli) xav tau ntau dua dov dhau thiab kev tswj xyuas qhov tseeb, yog li lawv raug nqi ntau dua ib kg. Cov phaj tuab (tshaj li 30 hli) siv cov slabs hnyav dua thiab raug nqi me ntsis ntxiv vim tias kev tsim khoom qeeb.
Quantity thiab Lead Time
Standard 4-6 lub lis piam tus me nyuam yog pheej yig tshaj. Rush xaj (hauv qab 3 lub lis piam) ntxiv $0.60–$1.00 ib kg.
Ntawv pov thawj thiab kuaj
Basic ASTM daim ntawv pov thawj suav nrog dawb. Tag nrho thib peb-kev tshuaj ntsuam xyuas (SGS, BV, lossis TÜV) lossis NORSOK M-630 ntxiv $ 0.40– $ 0.70 ib kg tab sis yuav tsum tau ua haujlwm rau kev ua haujlwm sab nrauv lossis lub nkoj siab.
Peb cov qauv kev them nqi pob tshab tso cai rau koj pom raws nraim qhov twg txhua duas mus - tsis muaj tus nqi zais.
2205 Duplex vs 316L vs Super Duplex Nqe Sib piv
Xaiv cov qib zoo yuav txuag tau nyiaj ntev -lub sij hawm. Nov yog ib sab ntshiab -los ntawm- sab saib:
Table 2: Nqe Ib Kg Sib Piv (Nruab nrab 15 mm Phaj, 5-tuj Order)
|
Qib |
Nqe ib kg (USD) |
Lub zog (Yield MPa) |
PREN Tus nqi |
Zoo tshaj rau |
20-Xyoo Nqi Txuag |
|
316L Austenitic UAS |
3.20 – 3.80 |
170–220 |
24–28 |
Ib puag ncig me me |
Lub hauv paus |
|
Duplex 2205 (S32205) |
5.10 – 5.90 |
450–550 |
32–36 |
Chloride + siab |
25–35 % |
|
Super Duplex 2507 |
7.80 – 9.20 |
550–700 |
40–45 |
Dej hiav txwv heev |
40% vs 316L |
S32205 muab 80-90% ntawm super duplex kev ua tau zoo ntawm 65% ntawm tus nqi. Nyob rau hauv feem ntau cov nroj tsuag tshuaj thiab offshore platforms, 2205 duplex phaj nqi ib kg muab tus nqi zoo tshaj.
Yuav ua li cas xam koj tag nrho 2205 phaj nqi?
Siv cov qauv no yooj yim:
Tag Nrho Tus Nqi=(Nqe ib kg) × (Tag nrho qhov hnyav hauv kg)
Kauj ruam-los ntawm- piv txwv
Koj xav tau kaum 15 hli tuab daim hlau, txhua 3000 hli × 1500 hli.
Luas alas=3 m × 1.5 m=4.5 m²
Luj ib m² (15 mm)=15 × 7.8=117 kg/m²
Nyhav ib phaj=117 × 4.5=526.5 kg
Tag nrho qhov hnyav rau 10 daim phiaj=5,265 kg
Nqe ib kg (10-tuj bracket)=$5.30
Tag nrho tus nqi=5,265 × 5.30=$27,904.50
Ntxiv freight ($ 0.80 - $ 1.50 ib kg) thiab koj muaj koj tus nqi tsaws hauv feeb.
Vim li cas peb lub Hoobkas muab qhov sib tw tshaj plaws 2205 Duplex Phaj Nqe Ib Kg?
Peb tswj tag nrho cov txheej txheem-los ntawm melting lub alloy mus rau qhov kawg dov-yog li peb tshem tawm cov cim distributor -ups. Peb cov nqi yog 15-25% qis dua US lossis European stockists thaum ua tau raws li cov qauv thoob ntiaj teb. Txhua lub phaj tau txais 100% kev kuaj ultrasonic thiab PMI pov thawj yam tsis muaj nqi ntxiv.
Cov neeg muas zaub uas sib piv quotes qhia peb peb duplex 2205 phaj nqi ib kg ua ke nrog ceev 15-25 hnub tus me nyuam yog unbeatable. Peb kuj muab kev pabcuam pub dawb los pab koj xaiv qhov tuab tuab uas txuag tau nyiaj ntau tshaj.
Lub tswv yim kom tau txais qhov zoo tshaj plaws Duplex 2205 Phaj Nqe Ib Kg
Order nyob rau hauv tag nrho cov thawv loads rau siab tshaj plaws luv nqi
Muab cov thicknesses sib txawv hauv ib qho kev txiav txim kom txo cov nqi teeb tsa
Thov zeb- ntug daim hlau es tsis txhob txiav- ntug thaum ua tau
Sib piv tag nrho cov nqi av (nqi + freight + dej num), tsis yog nqi ib kg
Npaj kom tau txais hnub no qhov tseeb duplex stainless hlau 2205 phaj nqi ib kg rau koj qhov project? Hu rau peb pab pawg muag khoom tam sim no ntawm+86 19339900211los yog Info@jnalloy.com. Xa koj cov thickness, qhov loj me, thiab ntau npaum li cas, thiab peb yuav rov qab cov lus hais ruaj khov nrog kev ntsuas qhov hnyav thiab tag nrho cov nqi hauv 24 teev.