Alloy 20 Forged Plug

Jun 27, 2025

Tso lus

Alloy 20 threaded plug, alloy 20 forged ntsaws, alloy 20 qhov ntsaws, astm A564 alloy 20 Forged Plug cov chaw tsim tshuaj paus hauv Suav.

 

Alloy 20 Forged Plug, tseem lees paub ua Nickel-Chromium Austenitic Alloy uas tau tsim rau cov kua qaub feem ntau ua rau cov kua qaub. Qhov kev kav dej superalloy muaj qee qhov zoo tsis kam mus rau kev tiv thaiv corrosion, kev ua yeeb yam hauv phosphoric uas muaj phosphoric, chlorides, thiab nitric acids. Alloy 20 forged plug raws li muaj niobium rau kev ua kom ruaj khov rau qhov tsis txaus ntseeg thiab kev tsim txiaj ntsig daws teeb meem. Nrog rau kev hwm thoob ntiaj teb zoo ntawm raw cov ntaub ntawv, peb kuj muab cov no li alloy 20 hauv cov khoom siv thickingized los ntawm peb cov neeg tau txais kev xav tau ntawm cov nqi ua lag luam. Alloy 20 forged ntsaws muab ob peb qhov zoo, suav nrog kev tiv thaiv zoo heev, muaj zog, thiab muaj peev xwm tiv thaiv kom kub & nias. Lawv kuj yooj yim ua haujlwm nrog thiab tuaj yeem siv tau, welded, thiab fab siv siv cov txheej txheem txheem. Alloy 20 forged ntsaws tawm pitting, crevice corrosion & kev nyuaj siab corrosion tawg.

 

Jinie Technology (Jiangsu) Co., Ltd yog tsim thiab muab alloy 20 ntsaws rau hauv cov nyiaj yuav tsum tau ua rau peb cov neeg siv khoom. Peb tab tom muab cov ntsaws rau hauv ntau cov ntaub ntawv, cov lus qhia tshwj xeeb, thiab qhov ntev li no rau peb cov neeg siv khoom. Peb muab cov no 150 plugs los ntawm kev siv sib txawv ntawm cov khoom siv raw, qib, hauv ntau qhov ntau thiab tsawg, duab. Raws li cov kev qhia tshwj xeeb muab los ntawm peb cov neeg siv nyiaj hwm, peb muab cov khoom lag luam hauv cov ntawv customized. Peb lub tuam txhab muaj ib pab neeg uas paub txog thiab cov kws tshaj lij uas tau tsim cov khoom lag luam zoo, Alloy 20 plugs hauv qhov ntau ntau. Peb tshawb xyuas txhua qhov tsis tas ntawm cov ntaub ntawv no ua ntej thov rau txhua yam khoom lag luam. Qhov no ua rau peb tau muab cov khoom lag luam zoo rau peb cov neeg siv khoom. Peb tab tom sim txhua lub tshuab, tshuaj thiab lub cev tsis muaj zog ntawm peb cov khoom ua ntej xa mus rau peb cov neeg siv khoom. Peb qib-qib alloy 20 plugs muaj ntau yam zoo xws li lub zog, ua haujlwm muaj peev xwm, weldability, fircability, fircility thiab ntau lwm tus uas ua rau lawv zoo tag nrho rau kev siv.

 

Alloy 20 feded plug splopifications

Cov lus qhia

ASTM B 564 \/ ASME SB 564

Tus qauv

ASTM, ASME, ANSI 16.11, MSS SP-79, 83, 95, 97, BS 3799

Qhov loj

1\/2 "nb rau 4" nb nyob rau hauv

Qho deb

15 nb t 0 100 nb

Hom

2000 lbs, 3000 lbs, 6010 lbs, 9000 lbs

Ntaus

Qhov (S \/ W) & Screwed (Scrd) - NPT, BSP, BSPT, Threaded Fittings

 

Alloy 20 forged Plug muaj hom

Alloy 20 Forged Hex Taub Hau Plug Standers

ASME SA182 CRMO Forged Plug

Alloy 20 Threaded Round Lub Taub Hau Plug

Alloy 20 Forged Plug

Alloy 20 fedged plug tus neeg lag luam hauv Is Nrias teb

Alloy 20 (Socket Weld Plug

Chrome Moly 2.4660 (Socket Weld Plard Chaw Tsim Tshuaj

ASME B16.11 CRMO Forged Plug

Alloy 20 Threading Plug

Alloy 20 Threading Plug

20 Alloy 2.4660 (socket weld ntsaws

ANSI B16.11 CRMO (Socket) Weld Plug

Alloy 20 N08020 xov rau plug

Alloy 20 feded (socks) weld ntsaws rau hauv Is Nrias teb

Alloy 20 feded plug exalter hauv Mumbai

A182 alloy 20 2. 4660 xov plug

Chrome moly xov xwm lub taub hau ntsaws cia

Alloy 20 forged txoj kev ntsaws

CRMO Forged \/ Socket Weld Plug Distributors

20 alloy 2.4660 qhov muag weld forged plug

Alloy 20 Threading Plug

ASTM A182 Alloy 20 N08020 xov rau cov ntsaws

Alloy 20 (Socket Weld Plug

Alloy 20 N08020 xov \/ (Socket Weld Plug Stockist

 

Tshuaj lom neeg tshuaj lom neeg ntawm Alloy 20 ntsaws

Alloy 20 ntsaws yog tsim ntawm ob peb lub ntsiab tseem ceeb, suav nrog:

Nickel (32. {{{00-38. {}}}}}}}}}}}.

Chromium (19. {{{{0-21. {{}}}}}}}}%): Tshwj xeeb hauv kev tiv thaiv corrosion, tshwj xeeb hauv oxidizing ib puag ncig.

Hlau (sib npaug): Ua cov qauv ntawm cov alloy, pab txhawb rau nws cov kev ntseeg siab.

Tooj liab (3. {{{0-4. {0%): txhim kho rau cov sulfuric acid.

Molybdenum (2. {{{0-3. {0%): txhim kho kom pitting thiab crevice corrosion.

Niobium (txog li 1. {{{0%): stampilizes lub alloy, tiv thaiv intergranular corrosion.

Lwm cov ntsiab lus: suav nrog carbon, mangelese, phosphorus, leej faj, thiab silicon hauv cov khoom me me kom zoo rau cov alloy cov khoom.

Qhov kev sib xyaw tshwj xeeb no, sib xyaw nrog lub ntsej muag-nruab nrab lo lo lus teb (FCC) Lattice tus qauv, muab alloy 20 nrog kev sib xyaw ua ke muaj zog, kev ua haujlwm nruj, thiab corrosion tsis kam.

 

NPT ALLOY 20 Xov Xwm Plug

Qhov loj me ntawm cov xov thread (BS 3799) (hauv hli)

Ntxhuab

Tus kav dej

Qhov loj

Qho ntev

(Tsawg kawg)

A

Plugs square taub hau

Plugs nruab nrab taub hau

Hex Plugs & Bushings

Siab txog
Xwm fab xwm meem
(Yam tsawg kawg nkaus)
B

Qhov dav
Flats
(Yam tsawg kawg nkaus)
C

Ntxhuab
Qhov dav
lub taub hau
E

Qho ntev
(Yam tsawg kawg nkaus)
D

Dav dawb
(Nominal)
F

Hex qhov siab (min.)

Kev chim
G

Daig
H

1/8"

9.7

6.6

7.1

10.4

35.1

11.2

–

6.4

1/4"

11.2

6.6

9.7

13.5

41.1

15.7

3.0

6.4

3/8"

12.7

7.9

11.2

17.5

41.1

17.5

4.1

7.9

1/2"

14.2

9.7

14.2

21.3

44.5

22.4

4.8

7.9

3/4"

15.7

11.2

15.7

26.9

44.5

26.9

5.6

9.7

1"

19.1

12.7

20.6

33.3

50.8

35.1

6.4

9.7

1-1/4"

20.6

14.2

23.9

42.9

50.8

44.5

7.1

14.2

1-1/2"

20.6

15.7

28.4

48.5

50.8

50.8

7.9

15.7

2"

22.4

17.5

33.3

60.5

63.5

63.5

8.6

17.5

2-2/2"

26.9

19.1

38.1

73.2

69.9

76.2

9.7

19.1

3"

28.4

20.6

42.9

88.9

69.9

88.9

10.4

20.6

4"

31.8

25.4

53.5

114.3

76.2

117.3

12.7

25.4

 

Cov Ntawv Thov thiab Kev Lag Luam siv Alloy 20 ntsaws

Alloy 20 Plug yog dav siv nyob rau hauv ntau yam kev lag luam vim nws cov kev lag luam zoo heev thiab kev kub siab - kub. Hauv kev lag luam ua lag luam kev ua lag luam, nws siv cov tshuaj tua hluav taws, cov khoom siv hluav taws xob, raws li nws tuaj yeem tiv thaiv cov roj acid, nitric acid, thiab lwm yam kev sib tawm suab. Hauv cov petrochemical thiab Refining kev lag luam, Alloy 20 ntsaws yog qhov tsim nyog rau kev tuav cov tshuaj ntau yam, uas pab tiv thaiv kev tiv thaiv xeb thiab abrasive ib puag ncig. Nyob rau hauv lub tsev tshuaj thiab kev lag luam ua khoom noj khoom haus, nws siv rau hauv cov khoom lag luam kom ntseeg tau tias muaj kev nyab xeeb thiab kev ua tau zoo rau pitting corrosion, thiab intergranular corrosion. Ib qho ntxiv, hauv kev lag luam fais fab thiab kev lag luam mary, alloy 20 ntsaws ntxiv rau kev ua tau zoo, xws li siv hauv kev hloov cua sov, thiab lwm yam khoom siv.

 

Xa kev nug
Los rau peb
Thiab pib koj rfqs tam sim no.
Tiv Tauj Peb