Nickel 200 (tsis yog tshaj 2004000 / W.NR. 2.4060 & 2.4066) yog kev lag luam ntshiab (99.6%) Whought Nickel. Qhov kawg 1% lossis tsawg dua yog tsim los ntawm cov hlau, nyiaj, manganese, tooj liab, carbon thiab sulfur hauv cov me me, ntsuas seb cov me nyuam ntsuas. Nws muaj cov khoom siv zoo thiab ua tau zoo heev rau ntau qhov chaw nruab nrab. Lwm cov yam ntxwv muaj txiaj ntsig ntawm lub alloy yog nws sib nqus thiab magnetos cov khoom siv, muaj cov khoom siv hluav taws xob, cov roj av tsawg cov ntsiab lus thiab cov roj av qis.
Cov corrosion tsis kam ntawm Nickel 200 ua rau nws muaj txiaj ntsig tshwj xeeb rau kev tswj cov khoom siv khoom ntawm kev tuav cov khoom noj, hluavtaws fibers, thiab caustic alkalies; Thiab tseem nyob rau hauv cov ntawv thov uas tsis kam rau corrosion yog qhov tseem ceeb. Lwm yam kev siv suav nrog cov tub yees duab xa tawm, cov hluav taws xob thiab qhov hluav taws xob, iberospace thiab cov foob pob mis.
Nickel 200 alloy tuaj yeem ua tau los ntawm txhua qhov kub ua haujlwm thiab ua haujlwm txias. Lub alloy tuaj yeem ua haujlwm kub ntawm 649 degree F) thiab 1232 Qib F), nrog kev sib tw hnyav f), nrog kev sib tw hnyav Annealing yog ua nyob rau ntawm qhov kub ntawm 704 degree (1300 degree f) thiab 871 degree (1600 degree f).
Nickel 200 Tshuaj lom neeg muaj pes tsawg leeg,%
|
Teem nqi |
C Tsawg dua lossis sib npaug |
Mn tsawg dua los yog sib npaug |
SI tsawg dua lossis sib npaug |
S tsawg dua los yog sib npaug |
Cu tsawg dua lossis sib npaug |
Fe tsawg dua lossis sib npaug |
Ni ntau dua lossis sib npaug |
|
Ni200 |
0.15 |
0.35 |
0.35 |
0.01 |
0.25 |
0.40 |
99.0 |
Nickel 200 lub cev muaj zog
Ntom ntom: 8.89 g / cm3
Melting taw tes: 1435-1446 degree
Nickel 200 Cov Khoom Siv Neeg Kho Tshuab
| Puab | Lub tensile | Paib lub zog | Elongation | Kev nyuaj | |||
| Lub zog | ({0. 2% offset) | Hauv 2 hauv. (51 | Brinell (3000 kg) | Rockwell B | |||
| ksi | MPa | ksi | MPa | mm),% | |||
| Qws thiab bar | |||||||
| Kub-ua tiav | 60-85 | 415-585 | 15-45 | 105-310 | 55-35 | 90-150 | 45-80 |
| Khaub thuas-kos | 65-110 | 450-760 | 40-100 | 275-690 | Oct -35 | 140-230 | 75-98 |
| Txias-kos, annealed lossis kub-tiav, annealed | 55-75 | 380-520 | 15-30 | 105-210 | 55-40 | 90-120 | 45-70 |
| Lub tais | |||||||
| Kub-Rolled | 55-100 | 380-690 | 20-80 | 140-550 | 55-35 | 100-150 | 55-80 |
| Kub-rolled, annealed | 55-80 | 380-550 | 15-40 | 105-275 | 60-40 | 90-140 | 45-75 |
| Daim ntaub | |||||||
| Tawv | 90-115 | 620-795 | 70-105 | 480-725 | 2月15日 | – | 90 min. |
| Ib qho tseem ceeb | 55-75 | 380-520 | 15-30 | 105-210 | 55-40 | – | 70 max. |
| Txoj cai | |||||||
| Dej txhawv | 90-130 | 620-895 | 70-115 | 480-795 | 2月15日 | – | 95 min. |
| Ib qho tseem ceeb | 55-75 | 380-520 | 15-30 | 105-210 | 55-40 | – | 64 Max. |
| Tubing | |||||||
| Ntxhov siab-relieved | 65-110 | 450-760 | 40-90 | 275-620 | 35-15 | – | 75-98 |
| Ib qho tseem ceeb | 55-75 | 380-520 | 12月30日 | 85-210 | 60-40 | – | 70 max. |
| Condenser thiab evaporator tubing | |||||||
| Ib qho tseem ceeb | 55-75 | 380-520 | 15-30 | 105-210 | 60-40 | – | 65 Max. 75-98 |
| Ntxhov siab-relieved | 65-110 | 450-760 | 40-90 | 275-620 | 35-20 | – | |
| Hlau, Khaub Thuam Txias | |||||||
| Ib qho tseem ceeb | 55-85 | 380-580 | 15-50 | 105-345 | 50-30 | – | – |
| No. 1 npau npau | 70-95 | 485-655 | 40-75 | 275-520 | 40-20 | – | – |
| Caij Nplooj Ntoos Hlav | 125-145 | 860-1000 | 105-135 | 725-930 | 2月15日 | – | – |
Nickel 200 cov qhab nia sib npaug
|
Lub hom phiaj |
Werkstoff.nr. |
Tsis yog |
JIS |
Bs |
Gost |
Ib tug kaum |
En |
|
Ni200 |
2.4066/2.4060 |
N02200 |
NW 2200 |
Na 11 |
HП-2 |
N-100M |
Ni 99.2 |
Astm specifications
|
YEEB / Raj |
Ntawv / phaj / Sawb |
Kev thaiv qhov rais |
Kev zam |
Kev sib haum |
|
ASTM B161 / B163 / B474 |
ASTM B162 |
ASTM B160 |
ASTM B564 |
ASTM B366 |
Cov Ntawv Thov
- Nickel alloy yeeb nkab haum rau fais fab nroj tsuag.
- Nickel alloy haum rau roj thiab roj kev lag luam.
- Nickel alloy forged haum rau kua dej.
- Luj tshib rau mis nyuj thiab ua zaub mov noj.
- Txauv Tshav Kub Kub.
- Kws ua lag luam kev lag luam.
- Threaded fitting rau pulp thiab ntawv kev lag luam.
- Aerospace thiab cov foob pob hluav taws.