304 Stainless Hlau Yeeb Nkab
304 Stainless hlau kav, 304 stainless hlau leeg, 304 stainless hlau seamless yeeb nkab, 304 stainless hlau tubing, 304 stainless hlau tubing, 30301 stainless hlau kav & cov hlua
304 yog lub hom phiaj dav dav uas tau siv dav siv los ua cov cuab yeej thiab cov khoom uas xav tau kev sib xyaw ua ke zoo (corrosion tsis kam thiab muaj peev xwm). Txhawm rau kom muaj qhov ua kom haum corrosion tsis kam ntawm stainless hlau, cov hlau yuav tsum muaj ntau dua 18% chromium thiab ntau dua 8% cov ntsiab lus npib tsib xee.
Qeb 304 Stainless hlau kav yog qhov hloov tau tshaj plaws thiab siv tau siv cov qauv hlau stainless hlau me me ntawm kev ua lag luam. Qib roj stainless 304 yog cov feem ntau siv hlau hauv kev lag luam. Stainless hlau 304 welded kav muaj lub zog siab dua vim yog lawv cov micruplex microstructure thiab nitrogen ntxiv. Cov yeeb nkab steel hlau cable 304 muaj cov khoom siv neeg kho kom zoo, tiv taus rau ntau cov neeg sawv cev corrosive. Tsis sib nqus nyob rau hauv anealed mob. Hardness thiab tensile lub zog yuav tau nce los ntawm kev ua haujlwm txias, tab sis hloov kho los ntawm cov ntsiab lus roj carbon txo qis rau
Muaj cov qauv sib txawv, qhov ntau thiab tsawg, qhov loj me, thiab cov qib rau cov roj av qub (Jiangsu) Co., Ltd, square, plaub fab, thiab cov khoom siv hydraulic ntawm seamless thiab weldedpipes. Lub stainless hlau 304 welded yeeb nkab yog ua los ntawm vuam ib txoj hlua nyias lossis daim ntawv ua ke. Jinie Technology (Jiangsu) Co., Ltd yog lub ntsej muag zoo {6} {{{8} {[} {tp Stainless Hlau 304 kav dej thiab hlab.
Txheem Tshwj Xeeb Rau Cov Hlau Stainless 304 kav & Tubes
|
Tus qauv |
ASTM / ASME A213, A249, A249, A369, A312, SA214, SA269, SA312, |
|
Txheej hauv lub taub |
6.00 mm od li 914.4 mm od, ntau thiab tsawg txog 24 "nb |
|
Qhov tuab |
0.3mm - 50 hli |
|
Ntaus |
Seamless / EFW / EFW / Welded / Fabricated / LSAWW PIPES |
|
Teem caij |
SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH160, XXS |
|
Seamless kav & Tubes Loj |
1/8 8 "NB - 24" NB |
|
ERW kav & Tubes Loj |
1/8 8 "NB - 36" NB |
|
EFW Kav & Tubes Loj |
6 "NB - 100" NB |
|
Qho ntev |
Ib leeg random, ob npaug random & xav tau ntev |
|
Puab |
Cov kav dej puag ncig / cov leeg, cov kav dej square, duab dhos, cov raj kab yeeb nkab / hlab, coiled hlab, "u" puab, hydraulic leeg |
|
Qhov kawg |
Tiaj kawg, beveled kawg, tsuj las |
Tus Hlau Stainless 304 kav & Tubes Tshuaj Muaj pes tsawg leeg
|
Teem nqi |
Tsis yog |
C Tsawg dua lossis sib npaug |
Mn |
P tsawg dua lossis sib npaug |
S tsawg dua los yog sib npaug |
SI tsawg dua lossis sib npaug |
Cr |
Ni |
|
TPTP304 |
S30400 |
0.08 |
2 |
0.045 |
0.03 |
1 |
18.0-20.0 |
8.0-11.0 |
Stainless hlau 304 kav dej thiab tubes cov khoom siv neeg kho tshuab
|
Cov Khoom Siv Neeg Kho Tshuab |
Tensile, Min, Ksi [MPa] |
Yield, Min, Ksi [MPa] |
Elongation,% (min) |
Hardness, HB (Max) |
|
TPTP304 |
75【515】 |
30【205】 |
35 |
192 |
SS 304 kav dej & tubing sib npaug qib kawm
|
Lub hom phiaj |
Werkstoff NR. |
Tsis yog |
JIS |
Bs |
Gost |
Ib tug kaum |
En |
|
TPTP304 |
1.4301 |
S30400 |
Sus304 |
304S31 |
08Х18Н10 |
Z7cn18-09 |
X5crni18-10 |
304 stainless hlau kav thiab cov leeg cov ntawv thov
304 Stainless hlau yeeb siv rau ntau txoj kev lag luam, suav nrog cov khoom noj thiab dej haus, tshuaj ntsuab, siv tshuaj lom neeg. Lub alloy muaj superior tiv taus rau corrosion, siab kub, thiab tshuaj lom neeg, ua rau nws zoo meej rau kev siv nyob rau hauv ib puag ncig muaj kev hnyav. SS 304 kav 'ntau yam kev siv suav nrog cov dej siv hluav taws xob muaj txiaj ntsig, kev hloov pauv cua sov, hws, evapators, thiab kev lag luam tshuab. Ib qho ntxiv, nws yog siv ua kom ua tau cov qauv kws ua haujlwm xws li tes ua, lub qhov rooj of elevator, thiab lub tsev facades.